Intambo yokuWelda yentsimbi engagqwaliyosisixhobo esibalulekileyo esisetyenziswayo kwimveliso yanamhlanje kunye nokulungiswa kwayo, kunye neeklasi ezithile ezenzelwe ukuhambelana kwezinto ezahlukeneyo kunye neemeko zenkonzo. I-EC410NiMo yenye yeeklasi ezikhethekileyo, ehlelwe njenge-martensitic stainless steel flux-cored wire. Ukwenziwa kwayo kwenzelwe ngokuchanekileyo ukudala ii-weldments eziqinileyo nezihlala ixesha elide ezinokumelana neemeko zokusebenza ezinzima, nto leyo eyenza ukuba ibe sisixhobo esibalulekileyo sokugcina nokuvelisa izinto kwimizi-mveliso.
Ukwakheka kweekhemikhali zale ntambo yokuWelda yeStainless Steel yeyona nto iphambili kwiimpawu zayo zokusebenza. Iqulethe i-11.0-12.5% yeChromium (Cr), enika inqanaba elisisiseko lokumelana nokugqwala. Ukongezwa kwe-4.0-5.0% yeNickel (Ni) kuphucula ukuqina kwaye kunceda kulawulo lwezakhiwo ezincinci, ngelixa i-0.40-0.70% yeMolybdenum (Mo) iphucula kakhulu ukumelana nokugqwala kwemingxuma kwaye yomeleza isinyithi se-weld. Le nkqubo ye-alloy elinganisiweyo yiyo echaza amandla okusebenza kwentambo.
Ngokuphathelele isicelo, i-EC410NiMoIntambo yokuWelda yentsimbi engagqwaliyoIlungele kakhulu ukuhlanganisa nokulungisa iintsimbi ezithile ze-martensitic stainless. Ilungelelaniswe kakuhle nokuwelda intsimbi ye-ASTM CA6NM kunye nothotho lweentsimbi ze-13%Cr-4%Ni. Oku kuhambelana kubalulekile ekuqinisekiseni ukuba ijoyinti ewelding ineempawu zoomatshini kunye nezokonakalisa ezifana nezo zezixhobo ezisisiseko, ngaloo ndlela igcina ukuthembeka kwenxalenye iyonke.
Iindlela ezisetyenziswayo zokusetyenziswa kwale Stainless Steel Welding Wire zibanzi kwaye zibalulekile kumashishini amaninzi. Isetyenziswa ngempumelelo ekulungiseni nasekugqumeni iindlela zeenqwelo-moya zecrane, imiqulu yokuprinta, kunye neeshaft zentsimbi. Iimpawu zayo zenza ukuba ifaneleke kakhulu ekwakheni kwakhona izinto ze-hydraulic turbine eziye zachaphazeleka kukukhukuliseka kwe-cavitation, kunye nezinye izinto zesakhiwo ezifuna indibaniselwano yokumelana nokugqwala kunye nokumelana nokuguguleka.
Ibanga le-EC410NiMo limele isisombululo esikhethekileyo nesisebenzayo ngaphakathi kolu didi lweIntambo yokuWelda yentsimbi engagqwaliyo. Ukwakheka kwayo kweekhemikhali ezithile kuthetha ngokuthe ngqo ukusebenza okuphezulu kwizicelo ezifuna amandla, ukusuka ekumelaneni nokuguga koomatshini ukuya ekumelaneni nohlaselo olunokutsha. Kwiinjineli kunye neengcali ezijongene nemingeni yokugcina okanye ukwenza izinto ezibalulekileyo, olu cingo lokuwelda lubonelela ngokhetho oluthembekileyo nolusebenzayo lokuqinisekisa ukulungiswa okuhlala ixesha elide kunye nomgangatho wokwakha.