Intambo ene-Flux-Cored EC410NiMo

Inkcazo emfutshane:

I-EC410NiMo yintambo ye-martensitic stainless steel flux-core ene-chemical composition equlethe i-11.0 – 12.5% ​​Cr, 4.0 – 5.0% Ni, kunye ne-0.40 – 0.70% Mo.

Iinkcukacha zeMveliso

Iithegi zeMveliso

Umgangatho ohambelanayo

GB/T 17853-2018 TS410NiMo-FC11

I-AWS A5.22M-2012 E410NiMoT1-1

Izinto ezilinganayo: 13Cr-4Ni (EN1.4313/UNS S41500)

Inkcazo

I-EC410NiMo yintambo ye-martensitic stainless steel flux-core ene-chemical composition equlethe i-11.0 – 12.5% ​​Cr, 4.0 – 5.0% Ni, kunye ne-0.40 – 0.70% Mo. Ifanelekile kuzo zonke iindawo.ukuwelda kwe-arc ene-flux-core(FCAW) ene-arc ezinzileyo, ukuchitheka okuncinci, kunye nokungasuswa kakuhle kwe-slag. Isinyithi esigciniweyo sinokumelana nokuguguleka okuhle, ukumelana nokuqhekeka, kunye neempawu zoomatshini. Kucetyiswa ukufudumeza kwangaphambili kwi-150 - 260℃, kwaye unyango lobushushu emva kokuwelda (PWHT) kwi-590 ~ 620℃ iyure e-1 (kulandele ukupholisa umoya, i-AC) luyafuneka emva kokuwelda.

Isicelo

Ilungele ukuwelda intsimbi ye-ASTM CA6NM kunye neentsimbi zochungechunge lwe-13%Cr – 4%Ni. Isetyenziselwa ukulungisa ii-hardfacing ze-crane rails, ii-printing rollers, ii-steel shafts, ii-hydropower components ezigutyungelwe yi-cavitation, kunye neendawo zesakhiwo ezifuna ukugqwala kunye nokumelana nokuguguleka.

Ukwakheka kweekhemikhali ze-Weld Metal (%)

I-elementi C Cr Ni Mo Mn Si P S Cu
Imfuneko ≤0.06 11.0-12.5 4.0-5.0 0.40-0.70 ≤1.00 ≤1.00 ≤0.040 ≤0.030 ≤0.75
Iziphumo zovavanyo 0.02 12.3 4.65 0.54 0.59 0.33 0.023 0.01 0.01

Iipropati zoomatshini zesinyithi esigciniweyo

Igama lovavanyo Amandla okuThamba (MPa) Ukwandiswa% I-X-Rey Uvavanyo lweMpembelelo(+20℃)J Ubunzima be-HB I-Hydrogen enyibilikayo (ml/100g)
Imfuneko ≥760 ≥15 Ibanga loku-1 – – ≤5
Iziphumo zovavanyo 845 19 Ibanga loku-1 60-90 250-310 ≤5

 

Ipharamitha yokuWelding ecetyiswayo

Umthombo wamandla: DC Reverse (DC-)

Ububanzi beWire kunye neCurrent:

I-Current ecetyiswayo:

Ububanzi bentonga (mm) 3.2 4.0 5.0
Ukuwelda Ngoku (A) 80-120 120-160 150-190

Isaziso

1. Bhaka i-electrode kwi-300℃ kangangeyure ngaphambi kokuba uyisebenzise ukususa umswakama.

2.Coca umhlwa, ioyile, kunye nokufuma kumphezulu wesinyithi osisiseko; sebenzisa umsebenzi omfutshane we-arc kwiintsimbi ezimxinwa ze-weld.

3. I-PWHT kufuneka yenziwe ngoko nangoko emva kokuwelda ukuze kuthintelwe ukuqhekeka.

 

 


  • Ngaphambili:
  • Okulandelayo: