I-AWS A5.22 E312T-1 Intambo egobileyo yentsimbi engenasici

Inkcazo emfutshane:

I-E312T-1 yintambo yentsimbi engagqwali ye-AISI 312 ene-flux-cored eneempawu zokusebenza ezilungileyo kakhulu.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-AWS A5.22 E312T-1 FLUX-CORED WIRE

Ukwenziwa kweeKhemikhali

Fe C Cr Ni Mo Mn Si P S N Cu
Ibhalansi 0.15 28.0-32.0 8.0-10.5 0.5 0.5-2.5 1.0 0.04 0.03 — 0.5

Ixabiso elinye liphezulu ngaphandle kokuba kuchazwe ngenye indlela.

Inkcazo kunye nezicelo
I-E312T-1 yintambo yentsimbi engagqwaliyo ye-AISI 312 enohlobo lwe-flux-core eneempawu zokusebenza ezilungileyo kakhulu. Ivelisa iidiphozithi ezixineneyo neziqinileyo ezinamandla aphezulu okutsalwa ngaphezu kwazo naziphi na iintsimbi ezingagqwaliyo ze-austenitic. Iidiphozithi ze-weld zihambelana neempawu kunye neempawu zoomatshini ze-AISI 312 base metal. Iidiphozithi ze-weld zimalunga ne-23 Rockwell C njengoko zisetyenziswa. Umatshini kufuneka wenziwe ngamanqanaba okutya acothayo njengoko iidiphozithi ze-weld zichasana nobushushu, ukugqwala kunye nokuguga. Ulwakhiwo olukhethekileyo lwe-metallurgical lolwe-ferrite oluxhonywe kwi-matrix ye-austenite. Oku kwenza iidiphozithi zichasane kakhulu nokuqhekeka.
Isetyenziselwa ukuwelda iintsimbi ezisisiseko zohlalutyo olufanayo kunye neentsimbi ezahlukeneyo. I-Inweld E312T-1 isebenza kakuhle kwiintsimbi ezimelana nokurhawuzelelwa, iintsimbi ze-manganese, iintsimbi eziqina, iintsimbi zasentwasahlobo, ipleyiti yezixhobo, iintsimbi ezivelisa isivuno esiphezulu kunye nokudibanisa iintsimbi ezishushu kakhulu kwiintsimbi ze-carbon kunye ne-alloy ephantsi. Lukhetho oluhle kakhulu njenge-underlay (umaleko we-buffer) kwiidiphozithi ezijongene nobunzima.
Iipropati zeSinyithi eziQhelekileyo zokuWelda
Amandla okuThamba e-AWS Spec: 95,000 psi Amandla okuKhula: 75,000 psi
Ukwandiswa: 35%

Iiparameters ezicetyiswayo
I-FCAW (DCEP – Electrode +) 100% CO2 okanye 75% – 95% Ar / Ibhalansi CO2

 

Ububanzi bentambo I-Voltage I-Amperage
0.045” 25-30 130-180
1/16” 24-29 160-250

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besibandakanyeka ekuveliseni ii-electrode zokuwelda,iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.