I-Nickel Alloy Welding Wire ERNiCrMo-3 Tig Wire

Inkcazelo emfutshane:

I-ERNiCrMo-3 lucingo oluphezulu lwe-nickel alloy oluphuhliswe ukuwelda kunye nokufakwa kwe-nickel-based alloys efana ne-625 okanye izinto ezifanayo.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Nickel AlloyUcingo lweWeldingUcingo lweTigI-ERNiCrMo-3

 

Iimpawu kunye nezicelo

Phezulunickelucingo lwe-alloy luphuhliselwe ukuwelda kunye nokugqumanickel-i-alloys esekelwe njenge-625 okanye izinto ezifanayo.

Iqinile izotywe ngendlela ekhethekileyo yokufumana iiwelds ezicocekile nezikumgangatho ophezulu ezinomthungo oqaqambileyo kunye ne-ductility egqwesileyo.

Intsimbi ye-weld ineempawu ezintle kakhulu zomatshini kumaqondo aphezulu kunye namaqondo aphantsi.

Ukuxhathisa okulungileyo kwi-pitting kunye noxinzelelo lwe-corrosion.

Ubushushu bokusebenza obucetyiswayo busuka kwi-cryogenic ukuya kuma-540°C.

Ngokuqhelekileyo isetyenziswa kushishino lwenkqubo yemichiza, ubunjineli baselwandle, amacandelo ereactor yenyukliya, i-aerospace kunye nangaphakathi kwezixhobo zolawulo longcoliseko njl.njl.

Iimathiriyeli ezisisiseko eziqhelekileyo

I-Inconel 601, i-Incoloy 800, i-alloy 625, i-alloy 825, i-Alloy 926*
* Uluhlu olubonisayo, hayi olupheleleyo

 

Imigangatho
EN ISO 18274 – Ni 6625 – NiCr22Mo9Nb
I-AWS A5.14 – ER NiCrMo-3

 

Ukuqulunqwa kwemichiza %

C%

Mn%

Fe%

P%

S%

Si%

Cu%

max

max

max

max

max

max

max

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ni%

Co%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

max

max

max

20.00

3.15

8.00

imiz

1.0

0.40

0.40

23.00

4.15

10.00

 

IiPropati zoomatshini
Tensile strength ≥760 MPa  
Unikeze Amandla ≥415 MPa  
Elongation ≥35%  
Amandla empembelelo ≥100 J  

Iipropati zoomatshini ziqikelelwa kwaye zinokwahluka ngokusekelwe kubushushu, igesi yokukhusela, iiparitha ze-welding kunye nezinye izinto.

 

Iigesi zokukhusela

EN ISO 14175-TIG: I1 (Argon)

 

Izikhundla zeWelding

EN ISO 6947-PA, PB, PC, PD, PE, PF, PG

 

Idatha yokuPakisha
Ububanzi Ubude Ubunzima  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg

 

 

Uxanduva: Ngelixa zonke iinzame ezifanelekileyo zenziwe zokuqinisekisa ukuchaneka kolwazi oluqulethweyo, olu lwazi lunokutshintshwa ngaphandle kwesaziso kwaye lunokuthi luthathwe njengelufanele ukukhokelwa ngokubanzi.

 