I-ERNiFeCr-1 iNickel Alloy Welding Wire, i-Nickel Tig Wire Filler Metal

Inkcazelo emfutshane:

I-alloy 825 (ERNiFeCr-1) yintambo ye-nickel-iron-chromium eyenza oku kukhetho olufanelekileyo kwiintlobo ezahlukeneyo zezicelo ezinzima.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Nickel AlloyUcingo lweWeldingUcingo lweTigI-ERNiFeCr-1

Imigangatho
EN ISO 18274 – Ni 8065 – NiFe30Cr21Mo3
I-AWS A5.14 – ER NiFeCr-1

 

Iimpawu kunye nezicelo

Ingxubevange 825 yi anickel-i-iron-chromium wire eyenza oku kukhetho olufanelekileyo kwiintlobo ezahlukeneyo zezicelo ezinzima.

Olu cingo lubonelela ngamanqanaba aphezulu okuxhathisa umhlwa kuzo zombini i-oxidising ephakathi kunye nokunciphisa imekobume.

Igqibelele ukugquma ukugquma apho kufuneka ukwakheka kweekhemikhali ezifanayo.

I-weldability egqwesileyo kunye nentsimbi ye-austenitic ye-weld ngokupheleleyo kunye nokumelana okuphezulu ngokuchasene noxinzelelo lwe-corrosion cracking kwimidiya equlethe i-ion chloride.

Ngokuqhelekileyo isetyenziswa kumashishini okulungisa imichiza, i-petrochemical, imveliso yephepha kunye nokuveliswa kwamandla njl.

 

Iimathiriyeli ezisisiseko eziqhelekileyo

I-G-X7NiCrMoCuNb 25 20, X1NiCrMoCuN25 20 6, X1NiCrMoCuN25 20 5, NiCr21Mo, X1NiCrMoCu 31 27 4, N08926, N08904, ALLOY 8025, N028 N028, UNS8, U. , 1.4529, 1.4539 (904L), 2.4858, 1.4563, 1.4465 , 1.4577 (310Mo), 1.4133, 1.4500, 1.4503, 1.4505, 1.4506, 1.4531, 1.4536, 1.4585, 1.4586 *
* Uluhlu olubonisayo, hayi olupheleleyo

 

Ukuqulunqwa kwemichiza %

C%

Mn%

Fe%

P%

S%

Si%

 

max

0.70

22.00

max

max

max

 

0.05

0.90

imiz

0.020

0.004

0.50

 

 

Cu%

Ni%

Al%

Ti%

Cr%

Mo%

 

2.30

43.00

max

1.00

22.00

3.00

 

3.00

46.00

0.20

1.20

23.50

3.50

 

 

IiPropati zoomatshini
Tensile strength ≥550 MPa  
Unikeze Amandla -  
Elongation -  
Amandla empembelelo -  

Iipropati zoomatshini ziqikelelwa kwaye zinokwahluka ngokusekelwe kubushushu, igesi yokukhusela, iiparitha ze-welding kunye nezinye izinto.

 

Iigesi zokukhusela

EN ISO 14175-TIG: I1 (Argon)

 

Izikhundla zeWelding

EN ISO 6947-PA, PB, PC, PD, PE, PF, PG

 

Idatha yokuPakisha
Ububanzi Ubude Ubunzima  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg

 

 

Uxanduva: Ngelixa zonke iinzame ezifanelekileyo zenziwe zokuqinisekisa ukuchaneka kolwazi oluqulethweyo, olu lwazi lunokutshintshwa ngaphandle kwesaziso kwaye lunokuthi luthathwe njengelufanele ukukhokelwa ngokubanzi.

 