I-Nickel Alloy Welding Wire ERNiCr-3 Mig Welding Wire

Inkcazelo emfutshane:

I-ERNiCr-3 isetyenziselwa i-welding ye-alloys 600, 601, 690, 800 kunye ne-800HT njl.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Nickel AlloyUcingo lweWeldingI-ERNiCr-3

Imigangatho
EN ISO 18274 - Ni 6082 - NiCr20Mn3Nb
I-AWS A5.14 – ER NiCr-3

 

Iimpawu kunye nezicelo

I-alloy 82 isetyenziselwa ukuwelda i-alloys 600, 601, 690, 800 kunye ne-800HT njl.

Intsimbi ye-weld edipozithiweyo inamandla aphezulu kunye nokunganyangeki kakuhle komhlwa, kubandakanywa ukuxhathisa kwe-oxidation kunye namandla okukrazuka okunyuka kumaqondo obushushu aphezulu.

Ilungele izicelo zokuwelda ezahlukeneyo phakathi ezahlukeneyonickeli-alloys, iintsimbi ezingenasici, iintsimbi zekhabhoni ezibandakanya ukugqithisa.

Ilungele usetyenziso olusuka kwi-cryogenic ukuya kumaqondo obushushu aphezulu okwenza le ngxubevange ibe yenye yezona zisetyenziswa kakhulunickelusapho.

Inxeba lomaleko oluchanekileyo lweempawu eziphezulu zokutyisa ucingo.

Ngokuqhelekileyo isetyenziselwa ukuvelisa amandla kunye namashishini epetrochemical njl.

Iimathiriyeli ezisisiseko eziqhelekileyo

Ingxubevange 600, ingxubevange 601, ingxubevange 690, ingxubevange 800, ingxubevange 330*
* Uluhlu olubonisayo, hayi olupheleleyo

 

Ukuqulunqwa kwemichiza %

C%

Mn%

Fe%

P%

S%

Si%

max

2.50

max

max

max

max

0.05

3.50

3.00

0.030

0.015

0.50

Cu%

Ni%

Co%

Ti%

Cr%

Nb+Ta%

max

67.00

max

max

18.00

2.00

0.50

imiz

1.00

0.75

22.00

3.00

 

Tensile strength ≥600 MPa
Unikeze Amandla ≥360 MPa
Elongation ≥30 MPa
Amandla empembelelo ≥100 MPa

Iipropati zoomatshini ziqikelelwa kwaye zinokwahluka ngokusekelwe kubushushu, igesi yokukhusela, iiparitha ze-welding kunye nezinye izinto.

 

Iigesi zokukhusela

EN ISO 14175-I1, I3

 

Izikhundla zeWelding

EN ISO 6947-PA, PB, PC, PD, PE, PF

 

Idatha yokuPakisha

Ububanzi

Ubunzima

Spool

IPallet Qty

1.00 mm

1.20 mm

I-15 Kg

I-15 Kg

BS300

BS300

72

72

Uxanduva: Ngelixa zonke iinzame ezifanelekileyo zenziwe zokuqinisekisa ukuchaneka kolwazi oluqulethweyo, olu lwazi lunokutshintshwa ngaphandle kwesaziso kwaye lunokuthi luthathwe njengelufanele ukukhokelwa ngokubanzi.

 


  • Ngaphambili:
  • Okulandelayo: