Intambo yokuWelda ye-AWS E310T1-1/4 yentsimbi engagqwaliyo ene-Flux-core

Inkcazo emfutshane:

I-E310T1-1/4 yintambo ekhuselweyo ye-flux-core eyenzelwe ukuwelda "kwindawo yonke" kwaye ingasetyenziswa ne-75%Ar / 25%CO2 okanye i-100% CO2 yegesi yokukhusela.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-E310T1-1/4 FLUX-CORED WIRE

UHLELO
Iklasi ye-AWS 5.22 E310T1-1/4 / ASME SFA A5.22 Iklasi ye-E310T1-1/4
I-UNS W31031 A#9 F#6

INKCAZELO
I-E310T1-1/4 yintambo ekhuselweyo ye-flux-core eyenzelwe ukuwelda "kwindawo yonke" kwaye ingasetyenziswa ne-75%Ar / 25%CO2 okanye i-100% CO2 yegesi yokukhusela.
Iiparameter zokuwelda kufuneka zilungiswe ukuze kuthintelwe ukuqhekeka okushushu.

ISICELO
I-E310T1-1/4 isetyenziswa kakhulu ekudibaniseni iintsimbi zesiseko ezifana nezo zifana neentsimbi ze-AISI 310.
I-E310T1-1/4 ingasetyenziselwa ukuwelda intsimbi yekhabhoni kwintsimbi engatyiwayo.
I-E310T1-1/4 ingasetyenziselwa ukuwelda okanye ukulungisa iintloko ze-alloy eziphezulu kunye nee-castings ezimelana nokugqwala zomxube ofanayo ngokubanzi.
Sebenzisa igalelo lobushushu obuphantsi – Cebisa iiJoules ezingama-30,000/Kwi-Uplimited.
Ziphephe iintsimbi ezigobileyo zokuwelda
Gcina ubushushu be-interpass bungaphantsi kwama-250°F
Zalisa zonke ii-craters zokuqala nezokuyeka ukuze uphephe ii-craters.

IKHEMISTRI EQHELEKILEYO (%)

C Cr Ni Mo Mn Si P S Cu
.10 25.9 20.4 .10 1.4 .82 .015 .005 .08

IIPROPATI ZOOMATSHINI EZIQHELEKILEYO

TENSILE STRENGTH 89,000 PSI
UKULONDOLOZWA KWI-2” 38%
UNYANGO LOBUSHUSHU AKUKHO

Qaphela: Iimpawu zoomatshini eziboniswe kusetyenziswa i-100% CO2

IIPARAMETHA ZOKWENZIWA KWEWELDING EZIQHELEKILEYO (ezisebenzisa i-CO2 eyi-100%)

I-DIA ye-.045”. I-FLAT & TIMA IFLETHI KUPHELA
ii-AMPS 130-190 120-250
IiVolts 24-29 25-29
I-WFS (IPM) 225-450 200-600

QAPHELA: Beka ngaphandle i-3/8”-1/2”
Yehlisa iivolts nge-2 xa usebenzisa i-75%Ar / 25%CO2

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besibandakanyeka ekuveliseni ii-electrode zokuwelda,iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.