I-AWS: E70T-6-H16, E70T6-A2-CS3-H16
I-AWS: Intambo ye-E70T-6-H16, E70T6-A2-CS3-H16 ene-Flux-cored self-shielded (FCAW-S). Yenzelwe ukuwelda kwindawo yayo, ene-high deposition kwi-carbon steel. Icetyiswa kwi-single okanye multiple pass, automatic kunye ne-semiautomatic welding.
IIMBONAKALO
Amanani aphezulu okufaka izinto kwiindawo ezithe tyaba nezithe tye
I-arc egudileyo kunye namanqanaba aphantsi okuchithachitha
Iyakwazi ukuvelisa iidiphozithi ze-weld ezineempawu zempembelelo ezingaphezulu kwe-27 J (20 f:Ibf) kwi--29°C (-20°F)
Iiwelda kwipleyiti enomhlwa kancinci okanye eqandisiweyo
Izicelo eziqhelekileyo
Ukwenziwa kweepleyiti ngokubanzi
Ukwenziwa kwesakhiwo, kuquka nezo zixhomekeke kwiimfuno zenyikima
Iindawo zokupakisha iinqanawa, ukuwelda izikhonkwane kwiinqanawa
Iibhulorho kunye neerigi zaselwandle
Ukuwelda phezu kwe-tack welds ezenziwe nge-stick electrode
UKWAKHIWA KWEDIPOZITHI
| Ulwahlulo | I-Polarity | %Ai | %B | %C | %Mn | %P | %S | %SI | I-Hydrogen esasazekayo |
| I-mL/100g Isinyithi Esihlanganisiweyo | |||||||||
| E70T-6- H8 | DC+ | Ubuninzi obuyi-0.03. | Ubuninzi be-1.75. | Ubuninzi obuyi-0.03. | Ubuninzi obuyi-0.03. | Ubuninzi obuyi-0.6. | Ubuninzi be-8.0. | ||
| I-E70T6- A2-CS3-H8 | DC+ | Ubuninzi obuyi-0.03. | Ubuninzi be-1.75. | Ubuninzi obuyi-0.03. | Ubuninzi obuyi-0.03. | Ubuninzi obuyi-0.6. | 8 ubuninzi. | ||
| Isiphumo Esiqhelekileyo | DC+ | 0.7-1.0 | 0.0019 | 0.05-0.08 | 1.19-1.61 | 0.02 | 0.01 | 0.17-0.28 | 5.1 |
I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besibandakanyeka ekuveliseni ii-electrode zokuwelda,iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.
Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.