Ii-electrode ze-AWS ECuSi CopperAlloy Electrode ezigqunywe nge-T207 Arc Copper Stick Welding Rods

Inkcazo emfutshane:

I-T207 (AWS ECuSi) yi-electrode ye-copper alloy ene-silicon bronze core kunye ne-low hydrogen sodium coating.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Electrode yokuWelda yeCopper kunye neCopper Alloy

T207                                                     

GB/T ECuSi-B

I-AWS A5.6 ECuSi

 

Inkcazo: I-T207 yi-electrode ye-copper alloy ene-silicon bronze core kunye ne-low hydrogen sodium coating. Sebenzisa i-DCEP (i-direct current electrode positive) eneempawu ezintle zoomatshini. Inokumelana okuhle nokugqwala kwii-inorganic acids ngaphandle kwe-nitric acid, uninzi lwee-organic acids kunye namanzi olwandle.

 

Ukusetyenziswa: Ifanelekile ukuwelda ubhedu, i-silicon bronze kunye nobhedu, ukuwelda umphezulu we-linings yemibhobho yoomatshini beekhemikhali, njl.

 

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

Cu

Si

Mn

Pb

I-Al+Ni+Zn

>92.0

2.5 ~ 4.0

≤3.0

≤0.02

≤0.50

 

 

Iimpawu zoomatshini zesinyithi esijijekileyo:

试验项目

Into yovavanyo

抗拉强度

Tensile strength

I-Mpa

延伸率

Ukwandiswa

%

保证值

Iqinisekisiwe

≥270

≥20

 

 

I-current ecetyiswayo:

Ububanzi bentonga

(mm)

3.2

4.0

5.0

Ukuwelda kwangoku

(A)

90 ~ 130

110 ~ 160

150 ~ 200

 

Isaziso:

Ukulumkela:

1. I-electrode mayibhakwe malunga nama-300°C kangangeyure e-1 ukuya kwezi-2 ngaphambi kokuba i-welding;

2. Ukufuma, ioyile, ii-oxides kunye nezinye izinto ezingcolileyo kumphezulu we-weldment kufuneka zisuswe ngaphambi kokuba kufakwe i-welding.

3. Xa kudityaniswa i-silicon bronze okanye i-surfacing welding kwintsimbi, akufuneki kufudunyezwe kwangaphambili. Ubushushu bokufudumeza kwangaphambili bokudityaniswa kwe-copper ecocekileyo bumalunga ne-450°C, kwaye ubushushu bokufudumeza kwangaphambili bokudityaniswa kwe-copper bumalunga ne-300°C;

4. Kufuneka kusetyenziswe ukuwelda okufutshane ngexesha lokuwelda. Ngexesha lokuwelda okunamaleya amaninzi, i-slag phakathi kwamaleya kufuneka ibe

isuswe ngokupheleleyo; emva kokuwelda, faka i-weld ngesando esithe tyaba ukuze ucocise iinkozo, ususe uxinzelelo, kwaye uphucule amandla kunye nokuqina kwe-weld.


  • Ngaphambili: