Iklasi ye-AWS E2209T1-1/T1-4Intambo yeFlux Core

IIMBONAKALO
Yenzelwe ukuwelda ngokwendawo, zombini zithe nkqo phezulu kwaye zilungele imibhobho esisigxina, kwaye ifanelekile kwiindawo zokuwelda ze-ASME 5G okanye ze-6G (umbhobho uhlala ungaphezulu kwe-150mm ububanzi, ungaphezulu kwe-15mm eludongeni).
Ukunyibilika kwesikhundla sonke
Ukususwa kwe-slag okugqwesileyo

Igesi yokukhusela
I-80% yeArgon / 20% yeCO2
I-CO2 eyi-100%

Ezona mpawu
• Ukunyibilikisa indawo yonke
• Iphakheji evaliweyo nge-vacuum
• Ukususwa kwenkunkuma ngendlela egqwesileyo
• Isatifikethi esibonisa ukwakheka kwediphozithi, inombolo ye-ferrite, kunye neempawu ze-charpy impact ezivavanyiweyo @ -196°C (-320°F)

Iklasi ye-AWS E2209T1-1/T1-4Intambo yeFlux CoreUkwenziwa kweeKhemikhali

C Cr Ni Mo Mn Si P S N Cu
.03 22.5 9.7 3.25 0.95 .60 0.03 .015 0.14 0.20
Iipropati zoomatshini beFlux Core Wire Mechanical zeKlasi ye-AWS E2209T1-1/T1-4
Tensile strength 120,000 psi
Unikeze Amandla 95,000 psi
Ukwandiswa (%) 26%
Iiparamitha ze-AWS Class E2209T1-1/T1-4 Flux Core Wire
Ububanzi I-WFS (ipm) I-Amperage IiVolts I-ESO (ngaphakathi) Izinga lokuFakelwa kweMali
(iikhilogram/iyure)
.045” 250 130 22 5/8-3/4” 5.4
300 160 24 5/8-3/4” 6.3
425 200 26 5/8-3/4” 9.2
780 270 32 5/8-3/4” 16.2
1/16” 150 170 23 3/4-1” 5.4
195 215 25 3/4-1” 7.0
240 250 26 3/4-1” 8.6
320 305 27 3/4-1” 11.5

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besibandakanyeka ekuveliseni ii-electrode zokuwelda,iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.


  • Ngaphambili:
  • Okulandelayo: