I-E316HT1-1 Intambo egobileyo yentsimbi engenasici
Ingcaciso yeMveliso
Iyahambelana nomgangatho: GB/T17853 E316T1-1
I-AWS A5.22 E316HT1-1
Iimpawu kunye nokusetyenziswa kwazo
1. Ngenxa yokuba inekhabhoni ethile, ifanelekile ukuwelda izixhobo zentsimbi engagqwaliyo ezimelana nobushushu obuphezulu;
2. Isebenza kakuhle kakhulu kwinkqubo yokuwelda efana ne-arc ezinzileyo, ukuchitheka kancinci, ukususwa kakuhle kwe-slag, ukondla ucingo oluzinzileyo, kunye nokuma okuhle;
3. Ngenxa yomxholo ophezulu weMo, ukumelana nokugqwala kunamandla;
4. Ifanelekile kwi-18%Cr-12%Ni-2%Mo welding kwi-petrochemical, kwi-pressure vessels, kwi-medical and food machines, kwi-fertilizer nakwezinye iindawo.
Ukwakheka kweekhemikhali (wt%)
| Ubunzima be-alloy% | C | Mn | Kwaye | Cr | In | Mo | P | S | Nge |
| GB/T | 0.08 | 0.5-2.5 | 1.0 | 17.0-22.0 | 11.0-14.0 | 2.0-3.0 | 0.040 | 0.030 | 0.50 |
| I-AWS | 0.04-0.08 | 0.5-2.5 | 1.0 | 17.0-22.0 | 11.0-14.0 | 2.0-3.0 | 0.040 | 0.030 | 0.75 |
| Ixabiso lomzekelo | 0.50 | 1.45 | 0.50 | 18.05 | 12.00 | 2.35 | 0.020 | 0.005 | 0.05 |
Ukuziphatha koomatshini
| Ukuziphatha koomatshini | Amandla okuvelisa i-MPa | Amandla okutsalwa kwe-MPa | Ukwandiswa% | Ixabiso lempembelelo J/℃ |
| GB/T | - | 520 | 30 | - |
| I-AWS | - | 520 | 30 | - |
| Ixabiso lomzekelo | - | 560 | 35 | - |
Uluhlu lwangoku olucetyiswayo: (DC+)
| Ububanzi bentambo yokuwelda (mm) | 1.2 | 1.6 |
| I-Voltage (V) | 22-36 | 26-38 |
| I-current (A) | 120-260 | 200-300 |
| Ukwandiswa okomileyo (mm) | 15-20 | 18-25 |
| Ukuhamba kwegesi (l/min) | 15-25 | 15-25 |
Amanyathelo okukhusela ukuwelda
1. Sebenzisa igesi ekhuselayo ye-CO2 enobunyulu obuyi-≥99.98% kunye nokuhamba kwegesi okuyi-20-25L/min.
2. Ubushushu obuphakathi kwemijelo: 16~100 ℃.
3. Xa kudityaniswa, kuyimfuneko ukuzikhusela emoyeni ukuze kuthintelwe ukuba iziphene zokudityaniswa zingasasazeki kwigesi yokukhusela. Ioyile, amanzi, njl. kwindawo yokudibanisa kufuneka zisuswe.
4. Sebenzisa ucingo lokuwelda ngokukhawuleza emva kokuvula iphakheji. Ukuba alusetyenziswanga ngokupheleleyo, thatha amanyathelo okukhusela ukufuma.
I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besibandakanyeka ekuveliseni ii-electrode zokuwelda,iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.
Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.