I-E71T-GS yi-electrode yentsimbi yekhabhoni, ene-flux-core esetyenziswa ngaphandle kwegesi yokukhusela yangaphandle. Le electrode yenzelwe ukuwelda intsimbi yekhabhoni e-thin-gauge, ukusuka kwi-3/16” ukuya kwi-22 gauge.
Izicelo eziqhelekileyo: ii-weldings ze-single-pass; le mveliso yenzelwe ukuwelda ngokufanelekileyo phezu kwezinto ezigayiweyo kwaye ingasetyenziswa nakwiindawo ezithile eziluminiyamu. I-E71T-GS ayifuni khuselo lwegesi lwangaphandle kwaye kufuneka iweldwe nge-DCEN (i-straight polarity).
| Iklasi ye-AWS: E71T-GS | Isiqinisekiso: AWS A5.20/A5.20M:2005 |
| I-alloy: E71T-GS | I-AWS/ASME SFA A5.20 |
| Indawo yokuWelda: H, F, V, O | Okwangoku: I-DCEN I-Polarity Ethe Tye |
| Amandla okuThanda aGuqukileyo, kpsi: | Imizuzu engama-86.4 (Ukuqhekeka kwesinyithi esisisiseko) |
| Uvavanyo lwe-Bend olukhokelwayo | Ihlangabezana neemfuno ze-AWS |
| Iiparameters zeWire eziqhelekileyo | |||||
| Ububanzi | Inkqubo | Ii-Amps | IiVolts | Isantya sokutya ngocingo | |
| in | (mm) | ||||
| .030″ | 0.8 | I-FCAW | 50 | 15 | 80 |
| I-FCAW | 100 | 16 | 225 | ||
| I-FCAW | 150 | 17 | 375 | ||
| I-FCAW | 175 | 17 | 445 | ||
| .035″ | 0.9 | I-FCAW | 75 | 15 | 70 |
| I-FCAW | 100 | 16 | 110 | ||
| I-FCAW | 150 | 17 | 180 | ||
| I-FCAW | 200 | 18 | 305 | ||
| .045″ | 1.2 | I-FCAW | 100 | 15 | 70 |
| I-FCAW | 150 | 16 | 120 | ||
| I-FCAW | 200 | 17 | 195 | ||
| I-FCAW | 225 | 17 | 245 | ||
| 1/6″ | 1.6 | I-FCAW | 150 | 17 | 60 |
| I-FCAW | 200 | 18 | 85 | ||
| I-FCAW | 250 | 18 | 135 | ||
| I-FCAW | 300 | 19 | 180 | ||
| 5/64” | .078 | I-FCAW | 200 | 19 | 60 |
| I-FCAW | 250 | 20 | 80 | ||
| I-FCAW | 300 | 21 | 115 | ||
| I-FCAW | 325 | 120 | 6.6 | ||
I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besibandakanyeka ekuveliseni ii-electrode zokuwelda,iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.
Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.