I-E71T-8-H8 A5.20, I-Carbon Steel Flux Cored Arc Welding Wire

Inkcazo emfutshane:

I-E71T-8-H8 yi-electrode ekhuselayo, intsimbi yekhabhoni, enomphetho we-flux. Yenzelwe ukuwelda ngaphandle kwegesi yokukhusela yekhabhoni kunye neentsimbi ezithile ze-alloy eziphantsi apho kufuneka khona ukuqina okuphezulu kobushushu obuphantsi.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Inkcazo:
I-E71T-8-H8 yi-electrode ekhuselayo, intsimbi yekhabhoni, enomphetho we-flux. Yenzelwe ukuwelda ngaphandle kwegesi yokukhusela yekhabhoni kunye neentsimbi ezithile ze-alloy eziphantsi apho kufuneka khona ukuqina okuphezulu kobushushu obuphantsi. I-slag eqandisayo ngokukhawuleza yenza kube lula ukuwelda kuzo zonke iindawo. Inokudluliselwa kwe-globular okugudileyo, imilo emihle yeentsimbi kunye ne-slag esuswa lula. I-E71T-8-H8 yenzelwe ukusetyenziswa kwezakhiwo ezifana nokwenziwa kwebhulorho, ukwakhiwa kweenqanawa kunye neenqanawa, kunye nezinye izinto ezisetyenziswa ngokubanzi.

Uhlu kunye nokuVunywa:
I-E71T-8-H8 ngokwe-AWS A5.20, i-ASME SFA 5.20
E71T8-A2-CS3-H8 nge-AWS A5.36, ASME SFA 5.36
I-AWS D1.8 I-Seismic, i-CWB E491T-8-H8, i-ABS 3YSA, i-DNV IIIYMS

Iingenelo:
Isebenza kwi-polarity ethe tye (DCEN) ngaphandle kwegesi yokukhusela yangaphandle.
Ukuqandisa ngokukhawuleza kwe-slag kwenza kube lula ukuwelda kuzo zonke iindawo.
Ibonisa ukudluliselwa kweglobular okugudileyo, ukuchitheka okuncinci kunye ne-slag esuswa lula.

Iimpawu eziqhelekileyo zoomatshini:
Amandla okuThatha okuGqibeleleyo (psi) 87,000
Amandla okuvelisa (psi) 64,000
Ipesenti yoLongation 27

Ulwakhiwo oluqhelekileyo lweDiphozithi (wt%):
CMnSi P S Al
0.210.720.20 0.010 0.005 0.55

Iiparameters zokuWelda ezicetyiswayo (DCEN):

Ububanzi I-WFS I-AMPEAGE I-VOLTAGE I-CTWD (NGAPHAKATHI)
1/16″ 120 165 17-18 5/8
  170 200 18-19 3/4
  220 235 20-21 1
  270 270 21-22 1
  350 310 23-24 1
         
.072″ 125 185 18-19 3/4
  175 220 20-21 1
  200 245 21-23 1
  225 265 22-24 1
  250 275 22-24 1
         
5/64″ 60 140 17-18 3/4
  100 210 18-19 3/4
  150 255 21-22 1
  200 300 22-23 1
  250 330 23-24 1

*Ezi parameters zingasetyenziswa kuzo zonke iindawo. Ukukwazi ukuwelda ngaphandle kwendawo kumanqanaba aphezulu ombane kuya kuxhomekeka kubukhulu bepleyiti kunye nesakhono sokuwelda.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besibandakanyeka ekuveliseni ii-electrode zokuwelda,iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.


  • Ngaphambili:
  • Okulandelayo: