Inkcazo emfutshane:

I-ER1100 iyakwazi ukumelana nokuhlaselwa ziikhemikhali kunye nokuguquguquka kwemozulu. Yingxubevange ethambileyo enokubumbeka kakhulu kwaye isetyenziswa kakhulu kwimveliso ye-thin gauge kunye ne-foil.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-ER1100 A5.10, i-aluminium kunye ne-aluminium aluminium aluminium aluminium aluminium aluminium electrodes kunye neentonga

I-ER1100 iyakwazi ukumelana nokuhlaselwa ziikhemikhali kunye nokuguquguquka kwemozulu. Yingxubevange ethambileyo elungele ukwakheka kwaye isetyenziswa kakhulu kwimveliso ye-thin gauge kunye ne-foil. Ineempawu ezintle zokumanzisa kwaye ikwasetyenziswa njengengxubevange yokuzalisa ngeenjongo zokuwelda. Uphawu olunqwenelekayo lwengxubevange kukugqitywa okukhanyayo okufunyenwe ngokufaka i-anodizing.

Izinto eziqhelekileyo ezisetyenziswayo: ukutshintshana kobushushu; izixhobo zokuphatha ukutya; iirivethi; ucingo lokubopha; ukwenza isinyithi

Iklasi ye-AWS: ER1100 Isiqinisekiso: AWS A5.10/ A5.10M:1999
I-alloy: ER1100 I-AWS/ASME SFA A5.10

 

Indawo yokuWelda:
F, V, OH, H
Okwangoku:
I-DCEP-GMAW
I-AC-GTAW

 

Iipropati eziqhelekileyo (njengoko zitshixiwe)

Ukuqhuba: 59% IACS (-12)
Amandla okuThamba, kpsi: 13
Umbala: Ngwevu
Indawo yokunyibilika 1215⁰F Ukuqina 1090⁰F Uxinano 0.098 lbs/cu Ngaphakathi.

I-Cystemi yeWire eqhelekileyo ngokwe-AWS A5.10 (amaxabiso alinganayo aphezulu)

I-Si + Fe Cu Mn Zn Okunye Al  
0.95 0.05-0.20 0.05 0.10 0.15 99.0 imizuzu  
Iiparameters zeWelding eziqhelekileyo
Ububanzi Inkqubo I-Volt Ii-Amps Igesi
in (mm)
.030 (.8) I-GMAW 15-24 60-175 I-Argon (cfh)
.035 (.9) I-GMAW 15-27 70-185 I-Argon (cfh)
3/64” (1.2) I-GMAW 20-29 125-260 I-Argon (cfh)
1/16” (1.6) I-GMAW 24-30 170-300 I-Argon (cfh)
3/32” (2.4) I-GMAW 26-31 275-400 I-Argon (cfh)
Ububanzi Inkqubo I-Volt Ii-Amps Igesi
in (mm)
1/16” (1.6) I-GTAW 15 60-80 I-Argon (cfh)
3/32” (2.4) I-GTAW 15 125-160 I-Argon (cfh)
1/8” (3.2) I-GTAW 15 190-220 I-Argon (cfh)
5/32” (4.0) I-GTAW 15 200-300 I-Argon (cfh)
3/16” (4.8) I-GTAW 15-20 330-380 I-Argon (cfh)

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besisenza ushishino lokuvelisa ii-electrode zokuwelda, iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.

 

 


  • Ngaphambili:
  • Okulandelayo: