I-AWS ER5183 i-Aluminiyam yokuwelda i-Aluminiyam i-MIG yokuwelda iintonga zeTig

Inkcazelo emfutshane:

I-ER5183 ifanelekile kwi-MIG ukuwelda i-aluminium magnesium alloy ukuba amandla aphezulu afunekayo kwaye ukuba isiseko sesinyithi si-5083 okanye i-5654 amandla okuqina aya kuba phezulu kakhulu.Isetyenziswa ngokubanzi ukuwelda i-aluminium magnesium alloy izakhiwo zeenqanawa, amaqonga angaphesheya kolwandle, iilocomotives & iinqwelo, iimoto, izitya, iinqanawa ze-cryogenic njalo njalo.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-ER5183 ifanelekile kwi-MIG ukuwelda i-aluminium magnesium alloy ukuba amandla aphezulu afunekayo kwaye ukuba isiseko sesinyithi si-5083 okanye i-5654 amandla okuqina aya kuba phezulu kakhulu.Isetyenziswa ngokubanzi ukuwelda i-aluminium magnesium alloy izakhiwo zeenqanawa, amaqonga angaphesheya kolwandle, iilocomotives & iinqwelo, iimoto, izitya, iinqanawa ze-cryogenic njalo njalo.Intsimbi yayo ye-weld inokumelana kakuhle ne-brine corrosion.

Isikhundla sokuwelda: F, HF, V

Uhlobo lwangoku: DCEP

ISAZISO:

Ukugcina ipakethe yocingo ikwimeko entle phambi kwewelding.

Yomibini imiphezulu ekufuneka idityaniswe nge-weldment kunye nocingo kufuneka icocwe kude nokungcola kweoyile, ukugquma kwe-oxide, ukufuma njalo njalo.

Ukufumana inkangeleko entle ye-weld kuyimfuneko ukutshisa isiseko sentsimbi ukuya kwi-100℃-200℃ phambi kokuba ukuwelda ukuba ubukhulu bayo buyi-10mm okanye ngaphezulu.

Kungcono ukubeka i-subplate phantsi kwendawo ye-weld ukuxhasa isinyithi esinyibilikisiweyo ukwenzela ukuba kuqinisekiswe ukungena ngokupheleleyo kwi-weldment.

Ngokwendawo yokuwelda kunye nobukhulu besiseko sentsimbi yegesi eyahlukileyo kufuneka ikhethwe, njenge-100% Ar, 75% Ar + 25% He, 50% Ar + 50% Yena, njl.

Iimeko ze-welding ezikhankanywe ngasentla zibhekisela kuphela kwaye kungcono ukwenza isiqinisekiso senkqubo ye-welding ngokweprojekthi ngaphambi kokuyibeka kwi-welding esemthethweni.

I-ER5183 UHLELO LWEKHEMICAL LWEMETALI EDEPOSITED (%):

SI FE CU MN MG CR ZN TI AI BE
Umgangatho ≤0.40 ≤0.40 ≤0.10 0.50-10 4.3-52 0.05-0.5 ≤0.25 ≤0.15 Ibhalansi ≤0.0003
Isiqhelo 0.08 0.12 0.006 0.65 4.75 0.130 0.005 0.080 Ibhalansi 0.0001

IIPROPATI ZOOMATSHINI BEMETALI EDEPOSITED (AW):

I-TENSILE STRENGTH RM (MPA) I-YELD STRENGTH REL (MPA) UBUDE A4 (%)
Isiqhelo 280 150 18

Ubungakanani & eCetyisiweyo yangoku kwiMIG (DC+):

WELDING WIRE DIAMETER (MM) 1.2 1.6 2.0
IWelding yangoku (A) 180-300 200-400 240-450
I-Welding Voltage (V) 18-28 20-20 22-34

UBUKHULU & OKUCETYHIWEYO NGE-TIG (DC¯):

WELDING WIRE DIAMETER (MM) 1.6-2.5 2.5-4.0 4.0-5.0
IWelding yangoku (A) 150-250 200-320 220-400