I-ERCUAL-A1 iAluminiyam yoNxibelelwano lweBronzi yokuWelding, iAluminiyam iTig Rod, iAluminiyam iMig yokuWelding

Inkcazelo emfutshane:

I-ERCuAl-A1 iAluminiyam yeBronze yokuWelding Wire yi-iron-free, i-aluminium ye-alloy ye-bronze ekhoyo kwi-spooled wire kunye ne-36 "yentonga yentsimbi engenanto yokuzalisa ukuze isetyenziswe kunye ne-gas metal-arc kunye ne-gas tungsten-arc iinkqubo zokuwelda ngokulandelelanayo.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-ERCuAl-A1 iAluminiyam yeBronze yokuWelding Wire yi-iron-free, i-aluminium ye-alloy ye-bronze ekhoyo kwi-spooled wire kunye ne-36 "yentonga yentsimbi engenanto yokuzalisa ukuze isetyenziswe kunye ne-gas metal-arc kunye ne-gas tungsten-arc iinkqubo zokuwelda ngokulandelelanayo.

I-ERCuAl-A1 Aluminium Bronze Welding Wire deposits isetyenziselwa ngokuyinhloko ukugqithisa ukuthwala kunye neendawo ezingaguqukiyo ezifuna ubunzima obumalunga ne-125 BHN kunye nokuxhathisa ukubola ngokukodwa kumanzi etyuwa, iityuwa zetsimbi, kunye nee-asidi ezininzi ezisetyenziswa ngokuqhelekileyo kwiindawo ezahlukeneyo kunye namaqondo okushisa.Le ingxubevange ayikhuthazwa ngokujoyina ekubeni idiphozithi akanalo utyekelo ukuba shushu mfutshane.

ERCuAl-A1 Aluminium Bronze Welding Wire Aluminium Bronze Welding Wire izicelo ziquka ityhubhu sheets, izihlalo valve, pickling hook, impellers, izityalo imichiza, kunye nepulp mills.

I-ERCUAL-A1 ALUMINUM I-ALUMINUM LWEBRONZE WOKWENGEZA IIMPAWU ZOMZIMBA NEZOBUCHWEPHESHE:

Iziqina-Ubushushu 1030℃
Ukuxinana 7.7kg/dm³
Elongation 40-45%
Ulwelo-Ubushushu 1040℃
Tensile strength 380-450N/mm²
Ukuqina kweBrinell 100HB

I-ERCUAL-A1 ALUMINIUM YOBRONZE WELDING INGCINGA YOKUPAKISHA:

MIG Ububanzi 0.8 - 2.0mm Ukupakishwa D100mm D200mm D300mm Ubunzima 1kg/5kg/12.5kg/13.6kg/15kg
0.030″-5/64″ 2lb/10lb/27lb/30lb/33lb
TIG Ububanzi 1.6 - 6.4mm Ubude 457mm / 914mm Ukupakishwa 5kg / ibhokisi 25kg / ibhokisi 10kg / iphakheji yeplastiki
1/16″ - 1/4″ 18″ / 36″ 10lb / ibhokisi 50lb / ibhokisi 10kg / iphakheji yeplastiki

Nceda uqaphele: Iimveliso ze-spools zamaplanga ze-500lb ziyafumaneka xa ziceliwe.

I-ERCUAL-A1 ALUMINUM UNCWALO LWEBRONZE WOKWESEKELA UDIDIWO LWEKHEMICAL (%):

Umgangatho ISO24373 GB/T9460 GB/T9460 I-BS EN14640 AWS A5.7 DIN 1733
Iklasi Cu6100 SCu6100 SCu6100A Cu6100 C61000 2.0921
Ingxubevange CuAl7 CuAl7 CuAl8 CuAl8 ERCuAl-A1 SG-CuAl8
Cu bal. bal. bal. bal. bal. bal.
Al 6.0-8.5 6.0-8.5 7.0-9.0 6.0-9.5 6.0-8.5 7.5-9.5
Fe - - ubuninzi 0.5 0.5 - ubuninzi 0.5
Mn 0.5 ubuninzi 0.5 ubuninzi 0.5 0.5 0.5 ubuninzi 1.0
Ni - - ubuninzi 0.5 0.8 - ubuninzi 0.8
P - - - - - -
Pb 0.02 - ubuninzi 0.02 0.02 0.02 ubuninzi 0.02
Si 0.2 ubuninzi 0.1 ubuninzi 0.2 0.2 0.1 ubuninzi 0.2
Sn - - ubuninzi 0.1 - - -
Zn 0.2 ubuninzi 0.2 ubuninzi 0.2 0.2 0.2 ubuninzi 0.2
enye 0.4 ubuninzi 0.5 ubuninzi 0.2 0.4 0.5 ubuninzi 0.4