I-AWS E309L-15 Iintonga zokuWelding zentsimbi, iSolder yentsimbi engenaStainless iArc Welding Electrode

Inkcazelo emfutshane:

I-A067 (AWS E309L-15) i-low-hydrogen sodium uhlobo lwe-ultra-low carbon Cr23Ni13 i-electrode yensimbi engenasici.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Stainless Steel WeldingI-Electrode

A067                                         

GB/T E309L-15

AWS E309L-15

Inkcazo: I-A067 i-low-hydrogen sodium uhlobo lwe-ultra-low carbon Cr23Ni13 i-electrode yensimbi engenasici.Sebenzisa i-DCEP (i-electrode echanekileyo yangoku) kwaye inokudityaniswa kuzo zonke izikhundla.Inomxholo wekhabhoni ephantsi, ngoko ke inokuxhathisa i-intergranular corrosion ebangelwa yi-carbide precipitation ngaphandle kwe-stabilizers ezifana ne-niobium kunye ne-titanium.

Isicelo: Isetyenziselwa uhlobo olufanayo lwesakhiwo sensimbi engenasici, intsimbi edibeneyo kunye nezixhobo zetsimbi ezikhethekileyo ekwenzeni i-synthetic fiber, i-petrochemical kunye nezinye izixhobo.Ingasetyenziselwa ukuvelela kwamaleko otshintsho kudonga lwangaphakathi lwemikhumbi yoxinzelelo lwesixhobo senyukliya kunye nokuweldiswa kwamalungu angaphakathi enqaba.

 

Ukwakhiwa kweekhemikhali zentsimbi edibeneyo(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Iimpawu zobuchwephesha bentsimbi ye-weld:

Into yovavanyo

Tensile strength

Mpa

Elongation

%

Iqinisekisiwe

≥520

≥25

 

yangoku eCetyisiweyo:

Intonga yobubanzi

(mm)

2.5

3.2

4.0

5.0

I-Welding yangoku

(A)

50 ~ 70

80 ~ 120

130 ~ 160

160 ~ 200

 

Isaziso:

1. I-electrode kufuneka ibhakwe ngeyure e-1 malunga ne-300 ℃ ngaphambi kokusebenza kwe-welding;

2. Kubalulekile ukucoca umhlwa, isikali se-oyile, amanzi, kunye nokungcola kwiindawo zokuwelda phambi kokuba udibanise.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Siye sabandakanyeka ekwenzenii-electrode ye-weldings, iintonga ze-welding, kwayeukuwelda izinto ezityiwayongaphezu kweminyaka engama-20.

Iimveliso zethu eziphambili ziquka insimbi engenasicii-electrode ye-weldings, carbon steel welding electrode, low alloy welding electrode, surfacing welding electrode, nickel & cobalt alloy welding electrode, mild steel & low alloy welding wires, steel stainless steel welding wires, flux cored cored wires, aluminiyam welding wires, submerged arc welding .iingcingo, i-nickel & ne-cobalt alloy welding ingcingo, iingcingo zokuwelda zobhedu, i-TIG & ne-MIG iingcingo zokuwelda, ii-electrode ze-tungsten, i-carbon gouging electrode, kunye nezinye izincedisi ze-welding & consumables.


  • Ngaphambili:
  • Okulandelayo: