Zithathele ingqalelo ngokupheleleyo ukwanelisa zonke iimfuno zabathengi bethu; fumana uphuculo oluqhubekayo ngokukhuthaza uphuculo lwabathengi bethu; khula ube liqabane lokugqibela elihlala lihleli labathengi kwaye wandise umdla wabathengi kwiFactory Price Welding Rod/Welding Material Welding Electrode (Aws E6013), Sisoloko sisebenzisana ekuphuhliseni imveliso entsha yobuchule ukuze ihlangabezane nesicelo sabathengi bethu kwihlabathi liphela. Joyina nathi kwaye masenze ukuqhuba imoto kube kukhuselekile kwaye kube mnandi kunye!
Zithwale ngokupheleleyo uxanduva lokwanelisa zonke iimfuno zabathengi bethu; fumana uphuculo oluqhubekayo ngokukhuthaza uphuculo lwabathengi bethu; yiba liqabane lokugqibela elihlala lihleli lentsebenziswano yabathengi kwaye wandise umdla wabathengi kubo bonke.I-China Welding Electrode kunye neNtonga yokuWelding, Iimveliso zethu zithunyelwa kwamanye amazwe kwihlabathi liphela. Abathengi bethu bahlala benelisekile ngumgangatho wethu othembekileyo, iinkonzo ezijolise kubathengi kunye namaxabiso akhuphisanayo. Injongo yethu "kukuqhubeka nokufumana ukuthembeka kwakho ngokuzinikela kwimizamo yethu ekuphuculeni rhoqo izisombululo kunye neenkonzo zethu ukuqinisekisa ukwaneliseka kwabasebenzisi bethu bokugqibela, abathengi, abasebenzi, ababoneleli kunye noluntu lwehlabathi esisebenzisana nalo".
ISICELO:
Ukuwelda kweentsimbi ze-9% Cr-1% Mo kunye neentsimbi ze-9% Cr – 2% Mo ezisetyenziselwa umbane kunye nesitya soxinzelelo oluphezulu.
IINKCAZELO:
I-PA-8016-B8 yi-electrode ye-hydrogen ephantsi enesinyithi se-weld esenziwe yi-9%Cr-1%Mo. Yenzelwe intsimbi eshushu kakhulu kunye neentsimbi ezisetyenziswa kwiinkonzo ze-hydrogen eshushu, ingakumbi kushishino lwe-petrochemical. I-electrode ingavunywa ngenxa yamandla ayo aphezulu okutsalwa, ukuqina okuhle kunye nokumelana nobushushu okukhulu.
AMANQAKU NGOKUSETYENZISWA:
1. Yomisa ii-electrode kwi-350-400°C malunga neyure enye ngaphambi kokuba uzisebenzise kwaye ugcine ii-electrode kwi-100-150°C emva kokuzomisa ngononophelo ukuze zingabi namanzi.
2. Sebenzisa indlela yokubuyela umva okanye ubethe i-arc kwipleyiti encinci yesinyithi elungiselelwe le njongo ukuthintela ukuvuthuza kwi-arc ukuqala.
3. Gcina i-arc imfutshane kangangoko.
4. Fudumeza kwi-100-150°C. Ubushushu obuza kusetyenziswa buyahluka ngokuhambelana nobukhulu bepleyiti kunye nohlobo lwentsimbi eza kudityaniswa.
5. Nika ingqalelo ukuba ungadluli kwi-heat-input efanelekileyo kuba i-heat-input egqithisileyo ibangela ukonakala kwexabiso lempembelelo kunye namandla emveliso yesinyithi esitshixiweyo.
IV. UKWAKHIWA KWEKHEMIKHALI OKUQHELEKILEYO KWESINYITHI ESIWELDWE (%):
| C | Si | Mn | Cr | Mo |
| 0.06 | 0.42 | 0.68 | 9.38 | 1.05 |
V. IIPROPATHI ZOKWENZA EZIQHELEKILEYO ZE-WELD STEAL:
| Amandla okuThamba N/mm2(Ksi) | Incopho yokuKhula N/mm2 (Ksi) | Ukwandiswa % | I-PWHT |
| 705 (102) | 560 (81) | 24 | 740°C x iyure e-1 |
VI. IINDLELA ZOKUWELDA: ZONKE IINDLELA
VII. UBUKHULU NOLUHLU LWANGOKU LUCETYISWAYO (AC/DC+):
| Ububanzi (mm) | 2.5 | 3.2 | 4.0 | 5.0 | |
| Ubude (mm) | 350 | 350 | 400 | 400 | |
| I-Ampere | Iflethi | 55 – 85 | 90 – 130 | 130 – 180 | 180 – 240 |
| V kunye ne-OH | 50 – 80 | 80 – 115 | 110 – 170 | 150 – 200 |
Zithathele ingqalelo ngokupheleleyo ukwanelisa zonke iimfuno zabathengi bethu; fumana uphuculo oluqhubekayo ngokukhuthaza uphuculo lwabathengi bethu; khula ube liqabane lokugqibela elihlala lihleli labathengi kwaye wandise umdla wabathengi kwiFactory Price Welding Rod/Welding Material Welding Electrode (Aws E6013), Sisoloko sisebenzisana ekuphuhliseni imveliso entsha yobuchule ukuze ihlangabezane nesicelo sabathengi bethu kwihlabathi liphela. Joyina nathi kwaye masenze ukuqhuba imoto kube kukhuselekile kwaye kube mnandi kunye!
Ixabiso leFektriI-China Welding Electrode kunye neNtonga yokuWelding, Iimveliso zethu zithunyelwa kwamanye amazwe kwihlabathi liphela. Abathengi bethu bahlala benelisekile ngumgangatho wethu othembekileyo, iinkonzo ezijolise kubathengi kunye namaxabiso akhuphisanayo. Injongo yethu "kukuqhubeka nokufumana ukuthembeka kwakho ngokuzinikela kwimizamo yethu ekuphuculeni rhoqo izisombululo kunye neenkonzo zethu ukuqinisekisa ukwaneliseka kwabasebenzisi bethu bokugqibela, abathengi, abasebenzi, ababoneleli kunye noluntu lwehlabathi esisebenzisana nalo".