Intambo yokuWelda eneCreed Flux, iBanga: Intambo yentsimbi engagqwaliyo engu-A 5.22 E308L T1-1

Inkcazo emfutshane:

Kwi-welding ye-Low Carbon 18-20% Cr/ 8-12% Ni steels ezinobuchule obuhle bokuwelda Ngenxa yokuba kukho i-ferrite, intsimbi yokuwelda ayinakuchaphazeleka kakhulu kukuqhekeka. Iipropati zoomatshini zingcono xa zikwimeko yokuwelda kwaye zinokumelana nokugqwala okungcono phakathi kwe-granular ngenxa yomxholo wekhabhoni ophantsi.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Flux Cored Ucingo lokuWelda, Udidi: A 5.22 E308l T1-1

Iinkcukacha zeMveliso

Izixhobo zocingo SS
Ubungakanani Ngomqulu Ngamnye 15 kg
Ukupakisha 15 kg ngepakethi nganye
Ibanga I-A 5.22 E308L T1-1
Uhlobo lokuPakisha I-spool ivalwe kwingxowa ye-polythene kwaye i-shrink isongelwe kwibhokisi ebotshelelweyo
Ubukhulu 1.2MM 1.6MM
Okwangoku 190-300A
Ulwandiso lweNtambo 20-25mm (inamathelayo)
Ubungakanani obufumanekayo 2.00mm, 2.4mm
I-Polarity Intambo ye-DC ilungile
Igesi yokukhusela Igesi ye-CO2 enesantya sokuhamba kwe-15-20 yeelitha/ngomzuzu
Iipropati zoomatshini bokuWelda I-UTS=520N/mm2 Umzuzu; Ubude(%)=35% umzuzu
Ikhemistri yesinyithi ewelding C= 0.035%,Mn=1.65%,P=0.02%,Si=0.50%,S=0.008%,Ni=9.50%,Cr=19.50%

Ingcaciso yeMveliso
Ucingo olune-cored flux yentsimbi engenasici olune-arc ezinzileyo negudileyo, olunokuqhekeka kakuhle kwe-slag

Izicelo:
Kwi-welding ye-Low Carbon 18-20% Cr/ 8-12% Ni steels ezinobuchule obuhle bokuwelda Ngenxa yokuba kukho i-ferrite, intsimbi yokuwelda ayinakuchaphazeleka kakhulu kukuqhekeka. Iipropati zoomatshini zingcono xa zikwimeko yokuwelda kwaye zinokumelana nokugqwala okungcono phakathi kwe-granular ngenxa yomxholo wekhabhoni ophantsi.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besibandakanyeka ekuveliseni ii-electrode zokuwelda,iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.