I-GB/T EZNiCu-1 (Z508) Cast Iron Welding Electrode Nickel-Copper Alloy (Monel) Core kunye neGraphitized Coating

Inkcazo emfutshane:

I-GB/T EZNiCu-1 (Z508) yi-electrode yokuwelda yentsimbi ephoswe ngentsimbi ene-nickel-copper alloy (Monel) core kunye ne-graphitized coating.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Ukuwelda kwentsimbi eyenziwe ngentsimbiI-electrode

I-Z508                                                     

GB/T EZNiCu-1

Inkcazo: I-Z508 yi-electrode yokuwelda yesinyithi ephoswe ngentsimbi enomphezulu we-nickel-copper alloy (Monel) kunye ne-graphitized coating. I-AC kunye ne-DC zinjongo ezimbini, i-arc ezinzileyo, kulula ukuyisebenzisa. Ukwenziwa kwayo kunye nokusebenza kwayo kokusika kusondele kwi-Z308, kodwa ngenxa yokuncipha okukhulu kwesinyithi esigciniweyo, ukumelana nokuqhekeka kuncinci. Amandla eejoyinti eziweldiweyo aphantsi, ngoko ke ayifanelekanga ukuwelda kwiindawo ezixineneyo.

Ukusetyenziswa: Isetyenziselwa ukulungisa ii-welding ze-grey iron castings ezingadingi amandla aphezulu.

 

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

C

Si

Mn

Fe

S

Ni

Cu

Ezinye

0.35 ~ 0.55

≤0.75

≤2.3

3.0 ~ 6.0

≤0.025

60 ~ 70

25 ~ 35

≤1.0

 

I-current ecetyiswayo:

Ububanzi bentonga

(mm)

3.2

4.0

5.0

Ukuwelda komsinga

(A)

90 ~ 110

120 ~ 150

160 ~ 190

 

Isaziso:

1. I-electrode kufuneka ibhakwe iyure e-1 malunga ne-150℃ ngaphambi kokuba isebenze nge-welding;

2. Xa udibanisa, kuyacetyiswa ukuba usebenzise indlela emxinwa, kwaye ubude be-weld nganye mabungadluli kwi-50mm. Ngoko nangoko faka i-weld ngesando esincinci ukuze unciphise uxinzelelo kwindawo yokulungisa i-weld kwaye uthintele ukuqhekeka emva kokudibanisa.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besibandakanyeka ekuveliseni ii-electrode zokuwelda, iintonga zokuwelda, kunyeukuwelda okusebenzisekayos iminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.

 


  • Ngaphambili:
  • Okulandelayo: