I-Nickel Alloy Wire Welding Wire ERNiCr-3 Nickel Tig Wire Filler Metal

Inkcazo emfutshane:

I-Alloy 82 (ERNiCr-3) isetyenziselwa ukuwelda ii-alloys 600, 601, 690, 800 kunye ne-800HT njl.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Nickel AlloyUcingo lokuWeldaUcingo lweTigI-ERNiCr-3

Imigangatho
EN ISO 18274 - Ni 6082 - NiCr20Mn3Nb
I-AWS A5.14 – ER NiCr-3

 

Iimpawu kunye nezicelo

I-alloy 82 isetyenziselwa ukuwelda ii-alloys 600, 601, 690, 800 kunye ne-800HT njl.

Isinyithi esifakwe kwi-weld sinamandla aphezulu kwaye simelana nokugqwala okuhle, kuquka ukumelana nokugqwala kunye namandla okuqhekeka kwe-creep kumaqondo obushushu aphezulu.

Ilungele ukusetyenziswa kwe-welding eyahlukeneyo phakathi kweentlobo ngeentlobo zezixhoboi-nickelii-alloys, iintsimbi ezingenasici, iintsimbi zekhabhoni kuquka nee-overlay.

Ifanelekile ukusetyenziswa ukusuka kwi-cryogenic ukuya kumaqondo obushushu aphezulu okwenza le alloy ibe yenye yezona zisetyenziswa kakhulu kusapho lwe-nickel.

Ngokwesiqhelo isetyenziswa kumashishini okuvelisa umbane kunye neekhemikhali njl.

Izinto ezisisiseko eziqhelekileyo

I-Alloy 600, i-Alloy 601, i-Alloy 690, i-Alloy 800, i-Alloy 330*
* Uluhlu olubonisa izinto, olungaphelelanga

 

 

Ukwakheka kweekhemikhali %

C%

Mn%

I-Fe%

P%

S%

I-Si%

 

ubuninzi

2.50

ubuninzi

ubuninzi

ubuninzi

ubuninzi

 

0.05

3.50

3.00

0.030

0.015

0.50

 

 

I-Cu%

I-Ni%

I-Co%

I-Ti%

I-Cr%

Nb+Ta%

 

ubuninzi

67.00

ubuninzi

ubuninzi

18.00

2.00

 

0.50

umzuzu

1.00

0.75

22.00

3.00

 

 

Iipropati zoomatshini
Tensile strength ≥600 MPa  
Unikeze Amandla ≥360 MPa  
Ukwandiswa ≥30 MPa  
Amandla empembelelo ≥100 MPa  

Iipropati zoomatshini ziqikelelwa kwaye zinokwahluka ngokusekwe kubushushu, igesi yokukhusela, iiparameter zokuwelda kunye nezinye izinto.

 

Iigesi zokukhusela

EN ISO 14175-TIG: I1 (Argon)

 

Iindawo zokuWelda

EN ISO 6947-PA, PB, PC, PD, PE, PF, PG

 

Idatha yokuPakisha
Ububanzi Ubude Ubunzima  
1.60 mm

2.40 mm

1000 mm

1000 mm

5 kg

5 kg

 

 

Uxanduva: Nangona kwenziwe yonke imizamo efanelekileyo ukuqinisekisa ukuchaneka kolwazi oluqulethweyo, olu lwazi lunokutshintsha ngaphandle kwesaziso kwaye lunokuthathwa njengolufanelekileyo kuphela kwisikhokelo ngokubanzi.