Izinto ezisetyenziswayo zokuWelda i-AWS A5.4 E310-15 i-Hydrogen Electrode ephantsi yeNtsimbi engagqwaliyo

Inkcazo emfutshane:

I-A407 (AWS E310-15) yi-electrode yentsimbi engagqwaliyo ye-austenitic ye-Cr26Ni21 ecocekileyo ene-hydrogen sodium coating ephantsi.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Ukuwelda kweNsimbi EngagqwaliyoI-electrode

A407                                   

I-GB/T E310-15

I-AWS A5.4 E310-15

Inkcazo: I-A407 yi-electrode yentsimbi engagqwaliyo ye-austenitic ye-Cr26Ni21 ecocekileyo ene-hydrogen sodium coating ephantsi. Sebenzisa i-DCEP (i-electrode yangoku ngqo) kwaye ingadityaniswa kuzo zonke iindawo. Isinyithi esigciniweyo sinokumelana okuhle kwe-oxidation phantsi kweemeko zobushushu eziphezulu ze-900 ~ 1100 ℃. Ekubeni isinyithi esigciniweyo siyi-austenite ecocekileyo, ukumelana nokuqhekeka kobushushu akulunganga njengokwesakhiwo se-duplex.

Ukusetyenziswa: Isetyenziselwa ukuwelda uhlobo olufanayo lwentsimbi engagqwaliyo engatshiyo, i-lining yentsimbi engagqwaliyo kunye nentsimbi eyahlukileyo, kwaye ingasetyenziselwa ukuwelda izakhiwo zentsimbi ezifana neCr5Mo, Cr9Mo, Cr13 kunye neCr28 ezinokuqina okuphezulu.

 

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

0.08 ~ 0.20

1.0 ~ 2.5

≤0.75

25.0 ~ 28.0

20.0 ~ 22.5

≤0.75

≤0.75

≤0.030

≤0.030

 

Iimpawu zoomatshini zesinyithi esijijekileyo:

Into yovavanyo

Tensile strength

I-Mpa

Ukwandiswa

%

Iqinisekisiwe

≥550

≥25

 

I-current ecetyiswayo:

Ububanzi bentonga

(mm)

2.0

2.5

3.2

4.0

5.0

Ukuwelda kwangoku

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Isaziso: I-electrode kufuneka ibhakwe iyure e-1 malunga nama-250℃ ngaphambi kokuba isebenze nge-welding.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besibandakanyeka kwimveliso yei-electrode yokuweldas, iintonga zokuweldakunyeizinto ezisetyenziswayo zokuweldakangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.

 

 

 


  • Ngaphambili: