Inkcazelo emfutshane:

I-AWS A5.23: I-ECM1, i-Summerged Arc Cored Wire yi-alloy ephantsi ye-alloy edibeneyo yocingo lwe-electrode ye-electrode ye-arc efakwe emanzini kwizicelo eziphezulu zamandla.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-AWS A5.23: I-ECM1, iiNcingo ze-Arc Cored eziNxibeleleyo

I-ECM1 yi-low-alloy composite ye-metal-cored wire electrode ye-arc ye-arc efakwe emanzini kwizicelo zamandla aphezulu.Kwaye idibana ne-AWS A5.23 chemistry i-M1 kwaye yenzelwe amanqanaba amandla okuqina ngaphezulu kwe-80 ksi.

IIMPAWU&INZUZO
• Iingcingo ezinomgangatho wesinyithi zinokubonelela ngamazinga aphuculweyo okubekwa xa kuthelekiswa neengcingo eziqinileyo kwiiamperages ezifanayo.
• Iingcingo ezine-metal-core zibonelela ngeeprofayili zokungena ezibanzi xa zithelekiswa neengcingo eziqinileyo kwiiparamitha zokuwelding ezinokuthelekiswa.
• Ibonelela ngokuqina okuhle kakhulu kobushushu obuphantsi kuzo zombini iimeko ezifana ne-welded kunye ne-stress- relieved
• Iimfuno zemichiza ye-Weld deposit ziyafana nezo ze-EM1 iingcingo eziqinileyo
• Ilungele ukusetyenziswa neentlobo ngeentlobo zokuguquguquka
• Ukubonelela ngesakhono sokwandisa isantya sokuhamba ukuze kuphuculwe imveliso
• Inceda ukunqanda ukutshisa xa udityaniselwa kwimisinga ephezulu kwiingcambu kunye nemathiriyeli ebhityileyo.
• Unceda ukunciphisa umngcipheko wokuqhekeka kwizicelo ezibalulekileyo okanye kwiindawo zenkonzo eziqatha
• Ifanelekile njengenye imveliso ephezulu kwiinkqubo ezininzi ezisebenzisa i-EM1 (okanye i-80 ksi efanayo) ucingo oluqinileyo.
• Ukubonelela ngezinto ezininzi ekuphuhlisweni kwenkqubo kunye nokwandisa ukusebenza kwesicelo se-welding

Amashishini
Ukwenziwa kwesakhiwo kunye nebhulorho, izixhobo ezinzima, ukuveliswa kwamandla, ukwakhiwa kweenqanawa, ngaphandle kolwandle
NGOKU
I-Electrode yangoku eNgqongileyo (i-DCEP), i-Electrode yangoku iNegative (DCEN), i-Alternating yangoku (AC)
UKUGCINA
Imveliso kufuneka igcinwe kwindawo eyomileyo, evaliweyo, kunye nokupakishwa kwayo kwangaphambili