I-AWS E7015-A1 I-Electrode yentsimbi enganyangekiyo bubushushu i-R107 Iintambo zokuWelda zeHydrogen eziphantsi ezinamathelayo

Inkcazo emfutshane:

I-R107 (AWS E7015-A1) yi-electrode yentsimbi enganyangekiyo bubushushu ye-pearlitic ene-hydrogen sodium coating ephantsi equlethe i-0.5% Mo.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Intsimbi Engagungqiyo Nobushushu yeMolybdenum kunye neChromiumUkuweldaI-electrode

R107                                                     

I-GB/T E5015-A1

I-AWS A5.5 E7015-A1

Inkcazo: I-R107 yi-electrode yentsimbi enganyangekiyo bubushushu ene-hydrogen sodium coating ephantsi equlethe i-0.5% Mo. Sebenzisa i-DCEP (i-electrode yangoku ngqo) kwaye ingadityaniswa kuzo zonke iindawo. I-weldment kufuneka ifudunyezwe ukuya kuthi ga kwi-90 ~ 110 ℃ ngaphambi kokuba idityaniswe.

Ukusetyenziswa: Isetyenziselwa ukuwelda imibhobho yebhoyila enobushushu obuphantsi kwama-510°C (njenge-15Mo, njl.njl.), kwaye ingasetyenziselwa ukuwelda intsimbi enamandla aphantsi.

 

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

C

Mn

Si

Mo

S

P

≤0. 12

0.50~ 0.90

≤0.50

0.40 ~ 0.65

≤0.030

≤0.030

 

Iimpawu zoomatshini zesinyithi esijijekileyo:

Into yovavanyo

Tensile strength

I-Mpa

Unikeze Amandla

I-Mpa

Ukwandiswa

%

Ixabiso lempembelelo (J)

Ubushushu obuqhelekileyo.

Iqinisekisiwe

≥490

≥390

≥22

≥47

 

Umthamo we-hydrogen osasazekileyo kwisinyithi esigciniweyo: ≤6.0mL/100g (indlela ye-glycerin)

Ukuhlolwa kwe-X-ray: Ibanga loku-1

 

I-current ecetyiswayo:

Ububanzi bentonga

(mm)

2.0

2.5

3.2

4.0

5.0

Ukuwelda kwangoku

(A)

40 ~ 70

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 

Isaziso:

1. I-electrode mayibhakwe iyure e-1 kwi-350℃ ngaphambi kokuba isebenze nge-welding;

2. Kubalulekile ukucoca umhlwa, isikali seoyile, amanzi, kunye nokungcola kwiindawo zokuwelda ngaphambi kokuba uwelda.