I-Filler Metal R407 (AWS E9015-B3) iPearlitic Heat-Resistant Steel Welding Electrode Low-Hydrogen Welding Rods Manual Metal Arc Electrodes

Inkcazelo emfutshane:

I-R407 (AWS E9015-B3) i-electrode yensimbi ye-pearlitic enganyangekiyo ukushisa kunye ne-low-hydrogen sodium coating equkethe i-2.5% Cr - 1% Mo.


Iinkcukacha zeMveliso

Iithegi zeMveliso

IMolybdenum kunye neChromium Molybdenum Ubushushu obunganyangekiyo kwintsimbi yeWelding Electrode

I-R407                                                     

I-GB/T E6015-B3

AWS A5.5 E9015-B3

Inkcazo: I-R407 i-electrode yensimbi ye-pearlitic echasene nokushisa kunye ne-low-hydrogen sodium coating equkethe i-2.5% Cr - 1% Mo. Sebenzisa i-DCEP (i-electrode ngqo yangoku i-positive) kwaye inokudityaniswa kuzo zonke izikhundla.I-weldment kufuneka ifudunyezwe ukuya kwi-200 ~ 300 ° C ngaphambi kwe-welding.

Isicelo: Isetyenziselwa ukuwelda ubushushu obuphezulu kunye noxinzelelo oluphezulu lwemibhobho kunye nobushushu bokusebenza obungaphantsi kwe-550 ° C, oomatshini bekhemikhali bokwenziwa, izixhobo zokuqhekeka kwepetroleum, njl.

 

Ukwakhiwa kweekhemikhali zentsimbi edibeneyo(%):

C

Mn

Si

Cr

Mo

S

P

0.05 ~ 0.12

0.50 ~ 0.90

≤0.50

2.00 ~ 2.50

0.90 ~ 1.20

≤0.030

≤0.030

 

Iimpawu zobuchwephesha bentsimbi ye-weld:

Into yovavanyo

Tensile strength

Mpa

Unikeze Amandla

Mpa

Elongation

%

Ixabiso lempembelelo (J)

ITemp yesiqhelo.

Iqinisekisiwe

≥590

≥490

≥15

≥47

Ivavanyiwe

600 ~ 680

≥500

18 ~ 21

 

Ukusasazwa kwe-hydrogen umxholo wentsimbi egciniweyo: ≤4.0mL/100g (indlela yeglycerin)

 

Ukuhlolwa kwe-X-reyi: I grade

 

yangoku eCetyisiweyo:

Intonga yobubanzi

(mm)

2.5

3.2

4.0

5.0

I-Welding yangoku

(A)

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 

Isaziso:

1. I-electrode kufuneka ibhakwe ngeyure eli-1 kwi-350 ℃ ngaphambi kokusebenza kwe-welding;

2. Kubalulekile ukucoca umhlwa, isikali se-oyile, amanzi, kunye nokungcola kwiindawo zokuwelda phambi kokuba udibanise.

 