I-AWS E9016-D1 I-Low Alloy Steel Welding Electrode J606 Iintambo zokuWelda ze-GB/T E6016-D1

Inkcazo emfutshane:

I-J606 (AWS E9016-D1) yi-electrode yentsimbi enamandla aphantsi eneentsimbi eziphantsi kunye ne-hydrogen potassium coating. Ingasetyenziselwa ukuwelda kwindawo yonke nge-AC kunye ne-DC. Uzinzo lokusebenza kokuwelda kwe-AC lungaphantsi kolo lokuwelda kwe-DC.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Electrode yeWelding yentsimbi ephantsi ye-Alloy

J606                                       

I-GB/T E6016-D1

I-AWS E9016-D1

Inkcazo: I-J606 yi-electrode yentsimbi enamandla aphantsi eneentsimbi eziphantsi kunye ne-hydrogen potassium coating. Ingasetyenziselwa ukuwelda kwindawo yonke nge-AC kunye ne-DC. Uzinzo lokusebenza kokuwelda kwe-AC lungaphantsi kolo lokuwelda kwe-DC.

Isicelo: Isetyenziselwa ukuwelda intsimbi yekhabhoni ephakathi kunye nezakhiwo zentsimbi enamandla aphezulu ahambelanayo, njenge-Q420, njl.

 

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

C

Mn

Si

Mo

S

P

≤0.12

1.25 ~ 1.75

≤0.60

0.25 ~ 0.45

≤0.035

≤0.035

 

Iimpawu zoomatshini zesinyithi esijijekileyo:

Into yovavanyo

Tensile strength

I-Mpa

Unikeze Amandla

I-Mpa

Ukwandiswa

%

Ixabiso lempembelelo (J)

-30℃

Iqinisekisiwe

≥590

≥490

≥15

≥27

Ivavanyiwe

620 ~ 680

≥500

20 ~ 28

≥27

 

Umthamo we-hydrogen osasazekileyo kwisinyithi esigciniweyo: ≤4.0mL/100g (indlela ye-glycerin)

Ukuhlolwa kwe-X-ray: Ibanga loku-1

 

I-current ecetyiswayo:

(mm)

Ububanzi bentonga

2.0

2.5

3.2

4.0

5.0

5.8

(A)

Ukuwelda kwangoku

40 ~ 70

70 ~ 90

90 ~ 120

140 ~ 180

180 ~ 220

210 ~ 260

 

 

Isaziso:

1. I-electrode mayibhakwe iyure e-1 kwi-350℃ ngaphambi kokuba isebenze nge-welding;

2. Kubalulekile ukucoca umhlwa, isikali seoyile, amanzi, kunye nokungcola kwiindawo zokuwelda ngaphambi kokuba kuweldwe;

3. Sebenzisa i-arc operation emfutshane xa udibanisa. Indlela yokuncamathela ebhityileyo ifanelekile;

4. Xa inxalenye ye-weld ityebile, kufuneka ifudunyezwe ibe ngaphezu kwe-150°C kwaye ipholiswe kancinci emva kokuyi-weld.

 