Intonga yokuWelda yentsimbi engagqwaliyo ye-E308L-17

Inkcazo emfutshane:

I-E308L-17 Yentonga Yokuwelda ye-Electrode ye-Stainless Steel Welding (i-Low C, i-18% Cr- 8% Ni)


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-E308L-17 Yentonga Yokuwelda ye-Electrode ye-Stainless Steel Welding (i-Low C, i-18% Cr- 8% Ni)

Ulwahlulo

EN IS03581-A:2016: E 19 9 L R 12

I-EN IS03581-B:2016: ES308L-17

I-AWS A5.4-2014: E308L-17

I-JISZ 3221-2013: ES308L-17

Inkcazo

-Isigqubuthelo senziwe ngohlobo lwe-titania yelayimu yokuwelda yentsimbi engagqwaliyo ye-18%Cr-8%Ni. (AISI 301, 302, 304, 308)

-Ukusebenza kakuhle kwe-welding ngenxa yesantya esiphezulu sokufakwa kwayo.

-Susa amanzi, umhlwa, ioyile nazo zonke izinto ezingaphandle kwindawo engenanto ngaphambi kokuba udibanise.

-Ukusetyenziswa kakuhle ngezicelo zangoku ezithe ngqo.

-Ukufudumeza kwangaphambili akuyomfuneko ngokubanzi.

-Hlaba kwakhona i-electrode kwi-250~350°C imizuzu engama-30~60 ngaphambi kokuba uyisebenzise.

Ukwakhiwa kweeKhemikhali Isinyithi esigciniweyo (%)
C Mn Si Cr Ni S P Mo Cu Fn
0.03 0.65 0.73 18.95 9.82 0.012 0.028 0.21 0.30 6.4

 

Ubungakanani kunye neKhona ecetyiswayo (i-AC okanye i-DC)
Ububanzi bentonga yokuwelda
(mm)
2.5 3.2 4.0 5.0
umsinga wokuwelda
(A)
55-80 90-130 110-150 140-180

Iimpawu zokusetyenziswa:

I-arc ezinzile kakhulu.

Ukususwa kakuhle kwe-slag.

Ukungena akunzulu kangako.

Ukumelana kakuhle nobushushu kunye nokugqwala.

Ukumelana kakuhle nokuqhekeka.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besisenza ushishino lokuvelisa ii-electrode zokuwelda, iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engama-22.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux ezikhuselweyo ngegesi, ii-wire welding ze-aluminium, i-submerged arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo..