Umthengisi wezinto ezisetyenziswayo zokuWelda i-EM14KS Intambo yokuWelda ye-Arc engaphantsi komhlaba, iiRodi zentsimbi yekhabhoni zokuWelda ye-Arc engaphantsi komhlaba

Inkcazo emfutshane:

I-EM14KS yi-electrode yentsimbi enomphetho wesinyithi, yekhabhoni yokwelulela i-arc engaphantsi komhlaba.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-EM14KS yi-electrode yentsimbi ehlanganisiweyo, yekhabhoni yentsimbi yokuwelda i-arc engaphantsi komhlaba. Yenzelwe ukuwelda i-carbon pass enye neninzi, kunye neentsimbi ezithile eziphantsi, kwiindawo ezithe tyaba nezithe tyaba. Khetha i-EM14KS iqulethe izongezo ezincinci ze-titanium eziphucula ubulukhuni bentsimbi yokuwelda kwaye zinceda ukugcina amandla emva kokunciphisa uxinzelelo. Le electrode kufuneka isetyenziswe kuphela ekuwelda i-arc engaphantsi komhlaba.

UHLELO:

I-EC1 nge-AWS A5.17, i-SFA 5.17.

IIMPAWU:

I-Select EM14KS yenzelwe ukuvelisa ikhemistri yediphozithi ye-weld elingana naleyo iveliswa yi-solid wire, ii-electrodes ze-EM14K. Uyilo lwe-cored wire lubangela amazinga aphezulu okufakwa kwe-deposition kune-solid wire xa isebenza kwinqanaba elifanayo langoku.

I-Select EM14KS ivumela ulawulo olungcono lokungena kweentsimbi kunentambo eqinileyo. Ipateni yokungena ye-electrode eneentloko ibanzi kwaye incinci kancinci, inciphisa ukutsha kwiindawo ezidlulayo okanye amalungu angalingani kakuhle.

ISICELO:

I-Select EM14KS ifanelekile kwezo zicelo ezibandakanya ukuwelda kwemithambo yoxinzelelo kunye neentsimbi zekhabhoni ezakhiweyo ezifana ne-A36, A285, A515, kunye ne-A516. Ifanele isetyenziswe kunye ne-neutral fluxes kwaye ingatshintshwa naphi na apho kusetyenziswa khona ucingo oluqinileyo, i-electrode ye-EM14K.

IKHEMISTRI YEDIPOZITHI EQHELEKILEYO:

Ubungakanani%

C

Mn

P

S

Si

Ti

.06

1.55

.015

.015

.55

.05

IIPARAMETHA ZOKUWELDA EZICETYISIWEYO:

5/64”

Ii-Amps
250

IiVolts
26-27

I-WFS (ipm)
90

I-ESO (ngaphakathi)
¾”-1¼”

Isantya sokuhla (lb/hr)
6.5

350

29-30

160

11

500

33-34

290

20

3/32”

275

28-29

80

1”-1¼”

8.5

450

32-33

155

15.5

600

37-38

245

24.7

1/8”

400

28-29

68

1”-1¼”

11.5

550

32-33

100

17

750

37-38

150

26.5

5/32”

425

30-31

45

1¼”-1½”

11.5

650

34-35

80

18.5

900

40-42

140

38