I-AWS: SFA 5.5 E9015-B3Ii-electrode zeentsimbi ezixhathisa ukuqhekeka

I-electrode ye-hydrogen ephantsi ebeka i-2.25Cr – 1Mo weld metal, ibonisa amandla amangalisayo kunye nokumelana nokuqhekeka kumaqondo obushushu aphezulu ukuya kuthi ga kwi-575 C. Isetyenziselwa ukuwelda intsimbi engashukumiyo ye-21⁄4 Cr-1 Mo kunye neentsimbi ze-Cr-Mo-V ezingashukumiyo kwi-hydrogen phantsi koxinzelelo kunye neentsimbi ezibunjiweyo ezinomxube ofanayo nentsimbi engashukumiyo. Izicelo eziqhelekileyo ziquka ukwakhiwa kwebhoyila yomphunga, ukuwelda imibhobho yomphunga kunye ne-super-heater, izityalo zamandla, indawo yokucocisa ioyile kunye nezityalo zeekhemikhali.

UKWAKHIWA KWEEKHEMIKHALI ZONKE ZESIMBI ESIWELDWE (%)

I-elementi C Mn Si P S Cr Mo
Ipesenti 0.05-0.12 0.5-0.9 ≤0.5 ≤0.030 0.022 2.0-2.5 0.9-1.2

IIPROPATI ZEZINTO EZINAMATHENI ZE-WELD STEAL

(I-PWHT: 690°C KWI-1 HR)

I-UTS YS Ukwandiswa
(MPa) (MPa) (L= 4d)%
≥590 550 ≥15

IDATHA YANGOKU NEYOKUPAKISHA: DC (+)

Ubungakanani (mm)

5×450

4×450

3.15×450

2.5×350

Uluhlu lwangoku (ii-Amps)

200-250

150-190

100-140

70-100

Ubungakanani (iiPC/ibhokisi)

35

55

75

100

Isilumkiso

1. Zomise kwakhona ii-electrodes kwi-250-300 C kangangeyure enye, ngokwendlela yethu eqhelekileyo yokuziqhelanisa.

2. Sebenzisa i-arc emfutshane kunye ne-stringer bead.


  • Ngaphambili:
  • Okulandelayo: