Iintambo zokuWelda ze-Aluminium ze-ER5356 kunye nee-Electrode

Inkcazo emfutshane:

I-ER5356 yi-alloy ye-aluminium yohlobo oluqhelekileyo ekhethwa ngenxa yamandla ayo aphezulu okucheba.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-ER5356 yi-alloy ye-aluminium yohlobo oluqhelekileyo edla ngokukhethwa ngenxa yamandla ayo aphezulu okucheba. Ukongeza, ikwabonelela ngokumelana nokugqwala okuhle kakhulu xa ivezwa emanzini anetyuwa. I-ER5356 kufuneka iqwalaselwe xa kudityaniswa iintsimbi ze-aluminium ezisisiseko ze-5000 series.

Izicelo eziqhelekileyo: ucingo lokugcwalisa i-welding

Iklasi ye-AWS: ER5356 Isiqinisekiso: AWS A5.10/ A5.10M:1999
I-alloy: ER5356 I-AWS/ASME SFA A5.10
Indawo yokuWelda:
F, V, OH, H
Okwangoku:
I-DCEP-GMAW
I-AC-GTAW
Iipropati eziqhelekileyo (njengoko zitshixiwe)
Ukuqhuba: 29% IACS (-0)/27% IACS (-H18)
Amandla okuThamba, kpsi: 38
Umbala: Mhlophe
Indawo yokunyibilika 1175⁰F Ukuqina 1060⁰F Uxinano 0.096 lbs/cu Ngaphakathi.
I-Cystemi yeWire eqhelekileyo ngokwe-AWS A5.10 (amaxabiso alinganayo aphezulu)
Si Fe Cu Mn Mg Cr Zn Ti Okunye AL
0.25 0.40 0.10 0.50-1.0 4.7-5.5 0.05-0.20 0.25 0.05-0.20 0.15 Intsalela
Iiparameters zeWelding eziqhelekileyo
Ububanzi Inkqubo I-Volt Ii-Amps Igesi
in (mm)
.030 (.8) I-GMAW 15-24 60-175 I-Argon (cfh)
.035 (.9) I-GMAW 15-27 70-185 I-Argon (cfh)
3/64” (1.2) I-GMAW 20-29 125-260 I-Argon (cfh)
1/16” (1.6) I-GMAW 24-30 170-300 I-Argon (cfh)
3/32” (2.4) I-GMAW 26-31 275-400 I-Argon (cfh)
Ububanzi Inkqubo I-Volt Ii-Amps Igesi
in (mm)
1/16” (1.6) I-GTAW 15 60-80 I-Argon (cfh)
3/32” (2.4) I-GTAW 15 125-160 I-Argon (cfh)
1/8” (3.2) I-GTAW 15 190-220 I-Argon (cfh)
5/32” (4.0) I-GTAW 15 200-300 I-Argon (cfh)
3/16” (4.8) I-GTAW 15-20 330-380 I-Argon (cfh)

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besisenza ushishino lokuvelisa ii-electrode zokuwelda, iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.

 

 


  • Ngaphambili:
  • Okulandelayo: