I-Tig kunye ne-Mig Wire A5.28 ER80S-D2, I-Low-alloy Steel Filler Metals ye-Gas Shielded Arc Welding

Inkcazo emfutshane:

I-ER80S-D2 yintambo eqinileyo yentsimbi ethambileyo esetyenziswa kwiimeko apho i-porosity iyingxaki okanye xa kufuneka ulwe nomxholo we-sulfur ephezulu okanye ikhabhoni kwisinyithi sakho esisisiseko.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-A5.28 ER80S-D2, Iintsimbi ze-A5.28 ER80S-D2, ezifakwe i-alloy esezantsi ze-Arc Welding ekhuselweyo yigesi

I-ER80S-D2 yintambo eqinileyo yentsimbi ethambileyo esetyenziswa kwiimeko apho i-porosity iyingxaki okanye xa kufuneka ulwe nomxholo we-sulfur ephezulu okanye ikhabhoni kwisinyithi sakho esisisiseko. Iqulethe amanqanaba aphezulu e-manganese kunye ne-silicon ukubonelela ngokumanzisa kakuhle kunye nokunyamezela umhlwa kunye nobunzima bokugqwala.

Izicelo eziqhelekileyo: usetyenziso olusemgangathweni we-x-reyi, ii-welds ezinamandla aphezulu, ii-boilers zomphunga, iitanki zoxinzelelo, imibhobho yegesi, utshintshiselwano lobushushu, imboni ye-petrochemical

Iklasi ye-AWS: ER80S-D2 Isiqinisekiso: AWS A5.28/A5.28M:2005
I-alloy: ER80S-D2 I-AWS/ASME SFA A5.28

 

Indawo yokuWelda: F, V, OH, H Okwangoku:
I-GMAW-DCEP

 

Amandla okuThamba, kpsi: imizuzu engama-80
Amandla okuvelisa, kpsi: imizuzu engama-68
Ukwandiswa %: imizuzu eli-17

I-Cystemical Wire Chemistry ngokwe-AWS A5.28 (amaxabiso alinganayo aphezulu)

C Mn Si P S Ni Mo Cu Okunye
0.07-0.12 1.60-2.10 0.50-0.80 0.025 0.025 0.15 0.40-0.60 0.50 0.50
Iiparameters zeWelding eziqhelekileyo
Ububanzi Inkqubo I-Volt Ii-Amps Igesi yokukhusela
in (mm)
.035 (0.9) I-GMAW 28-32 165-200 Ukudluliselwa kweSpray 98% Argon/2% Oxygen
.045 (1.2) I-GMAW 30-34 180-220 Ukudluliselwa kweSpray 98% Argon/2% Oxygen
1/16 (1.6) I-GMAW 30-34 230-260 Ukudluliselwa kweSpray 98% Argon/2% Oxygen
.035 (0.9) I-GMAW 22-25 100-140 Ukudluliselwa kweSekethe emfutshane 90% Helium/ 75% Argon / 25% CO2
.045 (1.2) I-GMAW 23-26 120-150 Ukudluliselwa kweSekethe emfutshane 90% Helium/ 75% Argon / 25% CO2
1/16 (1.6) I-GMAW 23-26 160-200 Ukudluliselwa kweSekethe emfutshane 90% Helium/ 75% Argon / 25% CO2
1/16 (1.6) I-GTAW 12-15 100-125 I-Argon eyi-100%
3/32 (2.4) I-GTAW 15-20 125-175 I-Argon eyi-100%
1/8 (3.2) I-GTAW 15-20 175-250 I-Argon eyi-100%

 