I-Nickel Alloy Welding Wire ERNi-1 yeNickel Tig Wire Filler Metal

Inkcazelo emfutshane:

I-ER-Ni1 isetyenziselwa ukuwelda kunye nokufakwa kwe-Nickel 200 kunye ne-Nickel 201 alloys.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Nickel AlloyUcingo lweWeldingUcingo lweTigERNi-1

Imigangatho
EN ISO 18274 – Ni 2061 – NiTi3
I-AWS A5.14 – ER Ni-1

 

Iimpawu kunye nezicelo

I-ER-Ni1 isetyenziselwa ukuwelda kunye nokufakwa kwe-Nickel 200 kunye ne-Nickel 201 alloys.

Ilungele ukujoyina iMonel alloys kunye nobhedu-nickeliialloyi kwiintsimbi zekhabhoni.

I-Ni1 iqulethe i-titanium eyaneleyo yokulawula i-weld-metal porosity kwiinkqubo ze-welding.

Ngokuqhelekileyo isetyenziswa kumashishini okulungisa imichiza, imveliso yefayibha eyenziweyo kunye nezixhobo zokulungisa ukutya njl.njl.

 

Iimathiriyeli ezisisiseko eziqhelekileyo

I-Nickel 200 kunye ne-201 *
* Uluhlu olubonisayo, hayi olupheleleyo

 

Ukuqulunqwa kwemichiza %
C% Mn% Fe% P% S% Si%  
max max max max max max  
0.05 0.80 0.70 0.030 0.010 0.75  
             
Cu% Ni% Co% Ti% Al%    
max 93.00 max 2.00 max    
0.20 imiz 1.00 3.50 1.00    

 

IiPropati zoomatshini
Tensile strength ≥410 MPa  
Unikeze Amandla ≥200 MPa  
Elongation ≥30 %  
Amandla empembelelo ≥100 J  

Iipropati zoomatshini ziqikelelwa kwaye zinokwahluka ngokusekelwe kubushushu, igesi yokukhusela, iiparitha ze-welding kunye nezinye izinto.

 

Iigesi zokukhusela

EN ISO 14175-TIG: I1 (Argon)

 

Izikhundla zeWelding

EN ISO 6947-PA, PB, PC, PD, PE, PF, PG

 

Idatha yokuPakisha
Ububanzi Ubude Ubunzima  
1.60 mm

2.40 mm

1000 mm

1000 mm

5 Kg

5 Kg

 

 