I-Electrode ye-Welding yentsimbi e-AWS E7018-G ene-Alloy Steel Welding Rods, Amandla esinyithi kunye ne-Hydrogen ephantsi

Inkcazo emfutshane:

I-J507FeNi (AWS E7018-G) yi-electrode yentsimbi e-alloy ephantsi enomgubo wentsimbi kunye ne-hydrogen coating ephantsi. Ingasetyenziselwa ukuwelda kwindawo yonke nge-AC kunye ne-DC


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Electrode yeWelding yentsimbi ephantsi ye-Alloy

J507FeNi                                                    

I-GB/T E5018-G

I-AWS E7018-G

Inkcazo: I-J507FeNi yi-electrode yentsimbi e-alloy ephantsi enomgubo wentsimbi kunye ne-hydrogen coating ephantsi. Ingasetyenziselwa ukuwelda kwindawo yonke nge-AC kunye ne-DC. Uzinzo lokusebenza kokuwelda kwe-AC lungaphantsi kolo lokuwelda kwe-DC

Isicelo: Isetyenziselwa ukuwelda intsimbi yekhabhoni ephakathi kunye neenqanawa zoxinzelelo lwentsimbi ezishushu kakhulu, ezifana ne-16MnDR, njl.

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

C

Mn

Si

Ni

S

P

≤0.08

0.80 ~ 1.30

≤0.65

1.20 ~ 2.00

≤0.030

≤0.030

 

Iimpawu zoomatshini zesinyithi esijijekileyo:

Into yovavanyo

 

Tensile strength

I-Mpa

 

Unikeze Amandla

I-Mpa

 

Ukwandiswa

%

 

Ixabiso lempembelelo (J)

-40℃

Iqinisekisiwe

≥490

≥390

≥22

≥54

 

Umthamo we-hydrogen osasazekileyo kwisinyithi esigciniweyo: ≤6.0mL/100g (indlela ye-glycerin)

Ukuhlolwa kwe-X-ray: Ibanga loku-1

 

I-current ecetyiswayo:

Ububanzi bentonga
(mm)

3.2

4.0

5.0

Ukuwelda kwangoku

(A)

90 ~ 120

140 ~ 180

170 ~ 210

 

Isaziso:

1. I-electrode kufuneka ibhakwe iyure e-1 malunga nama-350℃ ngaphambi kokuba isebenze nge-welding;

2. Kubalulekile ukucoca umhlwa, isikali seoyile, amanzi, kunye nokungcola kwiindawo zokuwelda ngaphambi kokuba uwelda.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besibandakanyeka kwimveliso yei-electrode yokuweldas, iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni,ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi ethambileyo kunye ne-low alloy, ii-wire welding zentsimbi engatyiwayo, ii-wire ze-flux ezikhuselwe yigesi, ii-wire welding ze-aluminium, i-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding zebrass, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.

 


  • Ngaphambili:
  • Okulandelayo: