I-Nickel Alloy Welding Wire ENiFe-Cl Mig Welding Wire

Inkcazo emfutshane:

Ucingo oluqinileyo lwe-Ferro-nickel olusetyenziselwa ukuwelda isinyithi esityhidiweyo kunye nesinyithi esithambileyo.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Nickel AlloyUcingo lokuWeldaI-ENiFe-Cl

Iimpawu kunye nezicelo

I-Ferro-i-nickelucingo oluqinileyo olusetyenziselwa ukuwelda isinyithi esityhidiweyo kunye nesinyithi esithambileyo.

Ifanelekile kwiindawo ezahlukeneyo zokudibanisa isinyithi esityhidiweyo, isinyithi esithambileyo, i-alloy ephantsi kunye neentsimbi ezingenasici.

Kucetyiswa ukuwelda ii-castings ezine-sulphur eninzi, i-phosphorus okanye i-lubricant engcoliswe yi-lubricant.

Inxeba lomaleko ochanekileyo ukuze kusetyenziswe iimpawu zokutyisa ucingo ezikumgangatho ophezulu.

Isetyenziswa rhoqo kwiintlobo ngeentlobo zezicelo zokulungisa nokuvelisa, kubandakanya ukwakha kwakhona imiphini, amavili, iindawo ezibalulekileyo phakathi kwentsimbi kunye nentsimbi ephosiweyo njl.njl.

Izinto ezisisiseko eziqhelekileyo

Intsimbi engwevu, ethambileyo, enamaqhuqhuva*
* Uluhlu olubonisa izinto, olungaphelelanga

 

Imigangatho
I-EN ISO 1071 – SC NiFe-1
I-AWS A5.15 – E NiFe-CI

 

Ukwakheka kweekhemikhali %
C% Mn% I-Si% P% S%
ubuninzi ubuninzi ubuninzi ubuninzi ubuninzi
2.00 0.80 0.20 0.03 0.03
I-Fe% I-Ni% I-Cu% I-Al%
umva. 54.00 ubuninzi ubuninzi
56.00 2.50 1.00

 

Iipropati zoomatshini
Tensile strength 400 – 579 MPa
Unikeze Amandla -
Ukwandiswa -
Amandla empembelelo -

Iipropati zoomatshini ziqikelelwa kwaye zinokwahluka ngokusekwe kubushushu, igesi yokukhusela, iiparameter zokuwelda kunye nezinye izinto.

 

Iigesi zokukhusela

EN ISO 14175 - I1, Ar + 1-2% O2

 

Iindawo zokuWelda

EN ISO 6947-PA, PB, PC, PD, PE, PF

 

Idatha yokuPakisha
Ububanzi
Ubunzima I-Spool IphalethiUbungakanani
1.20 mm 15 kg BS300 72