I-RBCuZn-A yoBronzi yaseNaval (RBCuZn-A) i-Copper-Zinc yokuqhola iWelding Wire Filler metal

Inkcazelo emfutshane:

I-ERCuSn-A Phos Bronze A lubhedu lwezinki oluqulethe malunga ne-5% yetoti kunye ne-0.35% ye-phosphorus eyongeziweyo njenge-deoxidizer esetyenziselwa ukuwelda ubhedu kunye nobhedu.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-RBCuZn-A i-Naval Bronze (i-RBCuZn-A) yintsimbi ye-copper-zinc brazing filler equlethe ixabiso elincinci le-tin ukuphucula amandla kunye nokuxhatshazwa kwe-corrosion kwi-weld deposit.Lukhetho oluhle xa iipropathi zamandla aphezulu zebronze evuthayo ephantsi zingafunwa.I-borax-boric acid flux iyafuneka ngokuqhelekileyo xa ubhobhoza le mveliso.

IKlasi ye-AWS: RBCuZn-A Isiqinisekiso: AWS A5.8/A5.8M:2011
Ingxubevange: RBCuZn-A ASME SFA A5.8

 

Indawo yokuGqama: H, V Uluhlu lweBrazing:
1330-1550⁰F

 

Amandla Okuqina, kpsi: 50
Elongation %, min: 30

 

Indawo yokunyibilika 1650⁰F Ukuqinisa 1610⁰F Ukuqina kweBrinell 70-90

IKhemistry yocingo eqhelekileyo ngokwe-AWS A5.8 (amaxabiso omnye ngawona aphezulu)

Cu Zn Sn Pb Al Okunye
57.0-61.0 Rem 0.25-1.00 0.05 0.01 0.50

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Siye sazixakekisa ekwenzeni ii-electrode zokuwelda, iintonga ze-welding, kunye nezinto ezisetyenziselwa ukuwelda iminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka i-electrode yentsimbi ye-welding, i-carbon steel welding electrode, i-alloy welding electrode, i-electrode ye-welding, i-nickel & ne-cobalt alloy welding electrode, intsimbi ethambileyo kunye ne-low alloy welding wires, i-welding steel wire, i-gas-shielded flux cored wire, iingcingo ze-aluminiyam, ukuwelda kwe-arc emanzini.iingcingo, i-nickel & ne-cobalt alloy welding ingcingo, iingcingo zokuwelda zobhedu, i-TIG & ne-MIG iingcingo zokuwelda, ii-electrode ze-tungsten, i-carbon gouging electrode, kunye nezinye izincedisi ze-welding & consumables.

 

 

 

 