Tyue Brand Best Welding Electrodes AWS A5.4 E320-16 for Stainless Steel

Inkcazelo emfutshane:

I-A902 (AWS E320-16) i-electrode yensimbi engenasici kunye ne-titanium-calcium coating.Ingasetyenziselwa zombini i-AC kunye ne-DC ngokusebenza okugqwesileyo kokusebenza.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Stainless Steel WeldingI-Electrode

A902

GB/T E320-16

AWS A5.4 E320-16

Inkcazo: I-A902 i-electrode yensimbi engenasici kunye ne-titanium-calcium coating.Ingasetyenziselwa zombini i-AC kunye ne-DC ngokusebenza okugqwesileyo kokusebenza.Intsimbi yayo egciniweyo inokumelana nokugqwesa okugqwesileyo kunye nokuxhathisa okuqinileyo kwi-oxidation kwaye isetyenziswa ngokubanzi kushishino lwemichiza, i-petroleum, kunye nezixhobo zokuvelisa i-hydrogen.

Isicelo: Isetyenziselwa ukuwelda i-Carpenter20Cb nickel alloy kwi-asidi ye-sulfuric, i-nitric acid, i-phosphoric acid kunye ne-oxidative acid corrosion medium.Ingasetyenziselwa ukuwelda intsimbi engafaniyo.

 

Ukwakhiwa kweekhemikhali zentsimbi edibeneyo(%):

C

Si

Mn

Cr

Ni

Mo

Cu

Nb

S

P

≤0.07

≤0.60

0.5 ~ 2.5

19.0 ~ 21.0

32.0 ~ 36.0

2.0 ~ 3.0

3.0 ~ 4.0

8 XC ~ 1.00

≤0.030

≤0.030

 

Iimpawu zobuchwephesha bentsimbi ye-weld:

Into yovavanyo

 Tensile strength

Mpa

Elongation

%

Iqinisekisiwe

≥550

≥30

 

yangoku eCetyisiweyo:

Intonga yobubanzi

(mm)

2.5

3.2

4.0

I-Welding yangoku

(A)

50 ~ 80

80 ~ 110

110 ~ 160

 

Isaziso:

  1. I-electrode kufuneka ibhakwe iyure enye malunga ne-150 ℃ phambi kokusebenza kwe-welding;
  2. Ngenxa yokuba ubunzulu bokungena bunzulu ngexesha lokuwelda kwe-AC, unikezelo lombane lwe-DC kufuneka lusetyenziswe kangangoko ukufumana ukungena nzulu.kwaye umsinga akufanele ube mkhulu kakhulu ukuphepha ubomvu bentonga ye-welding.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Siye sabandakanyeka ekwenzenii-electrode ye-weldings, iintonga ze-welding, kwayeukuwelda izinto ezityiwayongaphezu kweminyaka engama-20.

Iimveliso zethu eziphambili ziquka insimbi engenasicii-electrode ye-weldings, carbon steel welding electrode, low alloy welding electrode, surfacing welding electrode, nickel & cobalt alloy welding electrode, mild steel & low alloy welding wires, steel stainless steel welding wires, flux cored cored wires, aluminiyam welding wires, submerged arc welding .iingcingo, i-nickel & ne-cobalt alloy welding ingcingo, iingcingo zokuwelda zobhedu, i-TIG & ne-MIG iingcingo zokuwelda, ii-electrode ze-tungsten, i-carbon gouging electrode, kunye nezinye izincedisi ze-welding & consumables.

 