I-ECoCr-A (Cobalt 6) i-Cobalt Hardfacing kunye ne-Welding Electrode ekwaziyo ukunxiba

Inkcazelo emfutshane:

I-A5.13 ECoCr-C Cobalt Alloy Hardfacing Welding Rods isetyenziselwa ukuwelda iintloko zevalve, iiringi zokutywina zempompo yoxinzelelo oluphezulu kunye neenxalenye zezityuli.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-ECoCr-A (Cobalt 6) i-Cobalt Hardfacing kunye ne-Welding Electrode ekwaziyo ukunxiba

Uhlobo lwe-alloy: i-A5.13, i-Electrodes e-SOLID SURFACING kunye nee-Welding Rods, i-A5.13
I-ECoCr-A Cobalt Alloy 6 yeyona nto isetyenziswa kakhulu kwi-alloys esekwe kwi-cobalt enganyangekiyo kwaye ibonisa ukusebenza kakuhle okujikelezayo.Kuthathwa njengomgangatho woshishino lwezicelo zokumelana neenjongo eziqhelekileyo, unokumelana okugqwesileyo kwiindlela ezininzi zokuthotywa komatshini kunye neekhemikhali ngaphezulu komgangatho obanzi wobushushu, kwaye igcina inqanaba elifanelekileyo lobunzima ukuya kuthi ga kwi-500⁰C (930⁰F).Kwakhona kunokumelana okulungileyo kwimpembelelo kunye nokuguguleka kwe-cavitation.I-Cobalt Alloy 6 ifaneleka ngokufanelekileyo kwiinkqubo ezahlukeneyo zokuqina kwaye inokuguqulwa nge-carbide tooling.

Ukusetyenziswa okuqhelekileyo: iincakuba zokucheba;iivalve zokuqukuqela ulwelo;izikrufu ze-extrusion;amahlahla aqengqelekayo;ubushushu obuphezulu;umphezulu wevalvu

IKlasi ye-AWS: ECoCr-A Isiqinisekiso: AWS A5.13/A5.13M:2010
Ingxubevange: ECoCr-A ASME SFA A5.13

 

Indawo yeWelding:
F, V, OH, H
Okwangoku:
*NS

 

Amandla Okuqina, kpsi: *NS
Amandla eSivuno, kpsi: *NS
Elongation %: *NS

*NS ayichazwanga

IKhemistry yocingo eqhelekileyo ngokwe-AWS A5.13 (amaxabiso omnye ngawona aphezulu)

C Mn Si Cr Ni Mo Fe W Co Okunye
0.7-1.4 2.0 2.0 25-32 3.0 1.0 5.0 3.0-6.0 Rem 1.0