I-ECoCr-B (Cobalt 12) i-Cobalt Hardfacing kunye ne-Welding Electrode ekwaziyo ukunxiba

Uhlobo lwe-alloy: i-A5.13, i-Electrodes e-SOLID SURFACING kunye nee-Welding Rods, i-A5.13
I-ECoCr-B i-Cobalt Alloy 12 inokuthathwa njenge-alloy ephakathi phakathi kwe-Cobalt Alloy 6 kunye ne-Cobalt Alloy 1. Iqulethe iqhezu eliphezulu le-carbides eqinile, e-brittle kune-Cobalt Alloy 6, kwaye iye yanda ukuchasana nokukhukuliseka kwe-angle ephantsi, i-abrasion, kunye nobunzima obukhulu. i-sliding wear ngelixa igcina impembelelo efanelekileyo kunye nokuchasana kwe-cavitation.I-Cobalt Alloy 12 isoloko isetyenziselwa i-self-mated okanye iqhuba i-Cobalt Alloy 6 okanye i-1. Umxholo ophezulu we-tungsten ubonelela ngeempawu ezingcono zokushisa okuphezulu xa kuthelekiswa ne-Cobalt Alloy 6, kwaye ingasetyenziselwa kumaqondo okushisa ukuya kwi-700⁰C.I-Cobalt Alloy 12 isetyenziselwa ukusika izixhobo ezifuna ukuxhathisa i-abrasion, ukushisa kunye nokubola.

IiNkqubo eziQhelekileyo: imivalo yeesarha zamakhonkco;wabona amazinyo;I-extrusion iyafa

IKlasi ye-AWS: ECoCr-B Isiqinisekiso: AWS A5.13/A5.13M:2010
Ingxubevange: ECoCr-B ASME SFA A5.13

 

Indawo yeWelding:
F, V, OH, H
Okwangoku:
*NS

 

Amandla Okuqina, kpsi: *NS
Amandla eSivuno, kpsi: *NS
Elongation %: *NS

*NS ayichazwanga

IKhemistry yocingo eqhelekileyo ngokwe-AWS A5.13 (amaxabiso omnye ngawona aphezulu)

C Mn Si Cr Ni Mo Fe W Co Okunye
1.0-1.7 2.0 2.0 25-32 3.0 1.0 5.0 7.0-9.5 Rem 1.0

 