Stainless Steel WeldingI-Electrode

AF2209-15

GB/T E2209-15

AWS A5.4 E2209-15

Inkcazo: I-AF2209-15 yi-ultra-low carbon nitrogen-equkethe i-electrode yensimbi engenasici kunye ne-hydrogen ephantsi.Sebenzisa i-DCEP (i-electrode yangoku echanekileyo).Intsebenzo yokusebenza ilungile.Ngenxa yokuba iqulethe i-molybdenum kunye ne-nitrogen, kunye nomxholo wekhabhoni uphantsi kakhulu, isinyithi esifakiweyo sinokuxhathisa okulungileyo kokuqhekeka kunye nokuxhathisa ukubola, ngakumbi ukuxhathisa ukubola.

Isicelo: Isetyenziselwa kakhulu ukuwelda uhlobo olufanayo lwezixhobo zetsimbi ye-ultra-low carbon kwi-petroleum kunye ne-hydraulic industry.Okufana nokuwelda kwe-022Cr22Ni5Mo3N duplex yentsimbi engenasici.

 

Ukwakhiwa kweekhemikhali zentsimbi edibeneyo(%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤0.90

21.5 ~ 23.5

8.5 ~ 10.5

2.5 ~ 3.5

0.08 ~ 0.20

≤0.75

≤0.030

≤0.040

 

Iimpawu zobuchwephesha bentsimbi ye-weld:

Into yovavanyo

Tensile strength

Mpa

Elongation

%

Iqinisekisiwe

≥690

≥20

 

yangoku eCetyisiweyo:

Intonga yobubanzi

(mm)

2.5

3.2

4.0

5.0

I-Welding yangoku

(A)

50 ~70

80 ~ 110

130 ~ 150

160 ~ 200

 

Isaziso:

1. I-electrode kufuneka ibhakwe ngeyure eli-1 malunga ne-250 ℃ ngaphambi kokusebenza kwe-welding;

2. Kubalulekile ukucoca umhlwa, isikali se-oyile, amanzi, kunye nokungcola kwiindawo zokuwelda phambi kokuba udibanise.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Siye sabandakanyeka ekwenzenii-electrode ye-weldings, iintonga ze-welding, kwayeukuwelda izinto ezityiwayongaphezu kweminyaka engama-20.

Iimveliso zethu eziphambili ziquka i-electrode yentsimbi ye-welding, i-carbon steel welding electrode, i-alloy welding electrode, i-electrode ye-welding, i-nickel & ne-cobalt alloy welding electrode, intsimbi ethambileyo kunye ne-low alloy welding wires, i-welding steel wire, i-gas-shielded flux cored wire, iingcingo ze-aluminiyam, ukuwelda kwe-arc emanzini.iingcingo, i-nickel & ne-cobalt alloy welding ingcingo, iingcingo zokuwelda zobhedu, i-TIG & ne-MIG iingcingo zokuwelda, ii-electrode ze-tungsten, i-carbon gouging electrode, kunye nezinye izincedisi ze-welding & consumables.

 

 


  • Ngaphambili:
  • Okulandelayo: