I-Stainless Steel Welding Electrode AWS A5.4 E2553-16 Intonga ye-Electrodes eneTitanium-Calcium Coating

Inkcazelo emfutshane:

I-AF2553-16 (i-AWS E2553-16) yi-nitrogen ene-duplex ye-electrode yensimbi engenasici kunye ne-titanium-calcium coating.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Stainless Steel WeldingI-Electrode

AF2553-16

I-GB/T E2553-16

AWS A5.4 E2553-16

Inkcazo: I-AF2553-16 yi-nitrogen ene-duplex ye-electrode yensimbi engenasici kunye ne-titanium-calcium coating.Ingasetyenziselwa zombini i-AC kunye ne-DC ngokusebenza okugqwesileyo kokusebenza.Ngenxa yokuba iqulethe i-molybdenum kunye ne-nitrogen, kunye nomxholo wekhabhoni uphantsi kakhulu, isinyithi esifakiweyo sinokuxhathisa okulungileyo kokuqhekeka kunye nokuxhathisa ukubola, ngakumbi ukuxhathisa ukubola.

Isicelo: Isetyenziselwa i-welding duplex steel stainless kunye nomxholo wechromium malunga ne-25%, njenge-022Cr25Ni7Mo4N, 03Cr25Ni6Mo3Cu2N, UNS 32550 (Alloy255), njl.

 

Ukwakhiwa kweekhemikhali zentsimbi edibeneyo(%):

C

Mn

Si

Cr

Ni

Mo

Cu

N

S

P

≤0.06

0.5 ~ 1.5

≤1.0

24.0 ~ 27.0

6.5 ~ 8.5

2.9 ~ 3.9

1.5 ~ 2.5

0.10 ~ 0.25

≤0.030

≤0.040

 

Iimpawu zobuchwephesha bentsimbi ye-weld:

Into yovavanyo

Tensile strength

Mpa

Elongation

%

Iqinisekisiwe

≥760

≥15

 

yangoku eCetyisiweyo:

Intonga yobubanzi

(mm)

2.5

3.2

4.0

5.0

I-Welding yangoku

(A)

50 ~80

80 ~ 110

110 ~ 160

160 ~ 200

 

Isaziso:

1. I-electrode kufuneka ibhakwe ngeyure eli-1 malunga ne-250 ℃ ngaphambi kokusebenza kwe-welding;

2. Sebenzisa unikezelo lwamandla e-DC kangangoko kunokwenzeka, kwaye umsinga akufanele ube mkhulu kakhulu ukuphepha ukubomvu kwentonga ye-welding;

3. Ngaphambi kwe-welding, susa ioli, i-rust, isikali, umswakama kunye nezinye izinto ezingcolileyo kwindawo ye-welding.

 

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Siye sabandakanyeka ekwenzenii-electrode ye-weldings, iintonga ze-welding, kwayeukuwelda izinto ezityiwayongaphezu kweminyaka engama-20.

Iimveliso zethu eziphambili ziquka insimbi engenasicii-electrode ye-weldings, carbon steel welding electrode, low alloy welding electrode, surfacing welding electrode, nickel & cobalt alloy welding electrode, mild steel & low alloy welding wires, steel stainless steel welding wires, flux cored cored wires, aluminiyam welding wires, submerged arc welding .iingcingo, i-nickel & ne-cobalt alloy welding ingcingo, iingcingo zokuwelda zobhedu, i-TIG & ne-MIG iingcingo zokuwelda, ii-electrode ze-tungsten, i-carbon gouging electrode, kunye nezinye izincedisi ze-welding & consumables.

 

 


  • Ngaphambili:
  • Okulandelayo: