Ii-AWS A5.11 ENiCrFe-9 ii-Electrode ze-Nickel kunye ne-Nickel ze-Alloy Welding, ii-Electrode ze-Metal Arc ze-Manual, ii-Welding Rods

Inkcazo emfutshane:

I-Ni327 (AWS ENiCrFe-9) yi-electrode esekelwe kwi-nickel ene-hydrogen sodium coating ephantsi. Sebenzisa i-DCEP (i-electrode yangoku echanekileyo).


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Electrode yokuWelda yeNickel kunye neNickel Alloy

I-Ni327                                                     

GB/T ENi6094

I-AWS A5.11 ENiCrFe-9

Inkcazo: I-Ni327 yi-electrode esekelwe kwi-nickel ene-hydrogen sodium coating ephantsi. Sebenzisa i-DCEP (i-electrode yangoku ngqo)intle). Isinyithi esigciniweyo sinokumelana okuhle nokuqhekeka kuba i-weld inenani elithile lezinto ezixutywayo ezifana ne-molybdenum kunye ne-niobium.

Ukusetyenziswa: Isetyenziselwa ukuwelda ii-alloy ze-nickel ezifuna ukumelana nobushushu kunye nokugqwala, kwaye ingasetyenziselwa ukuwelda kunye nokugquma ezinye ii-alloy ezinzima ukuwelda kunye neentsimbi ezahlukeneyo.

 

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

C

Mn

Fe

Si

Cu

Ni

Cr

≤0.15

1.0 ~ 4.5

≤12.0

≤0.8

≤0.5

≥55.0

12.0 ~ 17.0

Nb + Ta

Mo

W

S

P

Okunye

 

0.5 ~ 3.0

2.5 ~ 5.5

≤1.5

≤0.015

≤0.020

≤0.50

 

 

Iimpawu zoomatshini zesinyithi esijijekileyo:

Into yovavanyo

Tensile strength

I-Mpa

Unikeze Amandla

I-Mpa

Ukwandiswa

%

Iqinisekisiwe

≥650

≥360

≥18

 

I-current ecetyiswayo:

Ububanzi bentonga

(mm)

3.2

4.0

Ukuwelda komsinga

(A)

90 ~ 110

110 ~ 150

 

Isaziso:

1. I-electrode kufuneka ibhakwe iyure e-1 malunga ne-300℃ ngaphambi kokuba isebenze nge-welding;

2. Kubalulekile ukucoca umhlwa, ioyile, amanzi kunye nokungcola kwiindawo zokuwelda ngaphambi kokuba uwelda.

 


  • Ngaphambili: