AWS ENiCu-7 Nickel Alloy Welding Rods Ni70Cu30 Nickel Based Welding Electrodes Manual Metal Arc Electrodes

Inkcazelo emfutshane:

I-Ni202 (AWS ENiCu-7) yi-Ni70Cu30 Monel alloy electrode ene-titanium calcium coating.Ingasetyenziselwa zombini i-AC kunye ne-DC.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Nickel kunye ne-Nickel Alloy Welding Electrode

Ni202                                                     

GB/T ENi4060

AWS A5.11 ENiCu-7

Inkcazo: I-Ni202 yi-Ni70Cu30 Monel alloy electrode ene-titanium calcium coating.Ingasetyenziselwa zombini i-AC kunye ne-DC.Intsimbi ediphozithiweyo inokumelana nokuqhekeka okulungileyo ngenxa yesiqulatho esifanelekileyo semanganese kunye ne-niobium.Inomsebenzi obalaseleyo we-welding kunye nokutsha kwe-arc okuzinzileyo, i-spatter encinci, ukususa i-slag ngokulula, kunye ne-weld entle.

Isicelo: Isetyenziselwa i-welding ye-nickel-copper alloy kunye ne-dissimilar steel, kwaye ingasetyenziselwa njengento yokugqithisa inguqu.

 

Ukwakhiwa kweekhemikhali zentsimbi edibeneyo(%):

C

Mn

Fe

Si

Nb

Al

Ti

Cu

Ni

S

P

≤0.15

≤4.0

≤2.5

≤1.5

≤2.5

≤1.0

≤1.0

27.0 ~ 34.0

≥62.0

≤0.015

≤0.020

 

Iimpawu zobuchwephesha bentsimbi ye-weld:

Into yovavanyo

Tensile strength

Mpa

Unikeze Amandla

Mpa

Elongation

%

Iqinisekisiwe

≥480

≥200

≥27

 

yangoku eCetyisiweyo:

Intonga yobubanzi

(mm)

2.5

3.2

4.0

Welding okwangoku

(A)

50 ~ 80

90 ~ 110

110 ~ 150

 

Isaziso:

1. I-electrode kufuneka ibhakwe ngeyure eli-1 malunga ne-250 ℃ ngaphambi kokusebenza kwe-welding;

2. Kubalulekile ukucoca umhlwa, i-oyile, amanzi, nokungcola kwiindawo zokuwelda phambi kokuba udiye.

 