Ii-electrode ze-ENiCrFe-3 zeNickel

Inkcazo emfutshane:

I-electrode ifaka isinyithi se-weld esingu-65Ni-20Cr-2Nb-1.5Mo.


Iinkcukacha zeMveliso

Iithegi zeMveliso

IKHOWUDI YE-ISO YE-EN: 14172:ENi6082

I-Electrode ifaka isinyithi se-weld esingu-65Ni-20Cr-2Nb-1.5Mo. Isinyithi se-weld esisemgangathweni we-radiographic esineempawu eziphezulu. Sifanelekile kwii-alloys ze-welding ze-compositions ezifanayo nazo, kwi-overfacing steel ene-Nickel-Chromium-Iron alloy xa umxholo ophezulu weManganese ungonakalisi, kwicala le-welding clad ye-Nickel Chromium-Iron clad kunye neendibaniselwano zesinyithi ezahlukeneyo. Sifanelekile kwiipleyiti ze-forge overlay. Sicetyiswa ngokukodwa kwi-welding ye-9% Ni Steels kwinkonzo ye-cryogenic. Sikwasetyenziselwa ukuwelda ii-alloys ze-Nickel-Chromium ezisetyenziselwa usetyenziso lobushushu obuphezulu njengezinto zokufudumeza i-furnace kunye neetyhubhu zokuhlaziya.

UKWAKHIWA KWEEKHEMIKHALI OKUQHELEKILEYO KWESINYITHI ESIWELDWEYO

I-elementi C Mn Si Cr Ni Fe Nb Cu Ti S P
Ipesenti ≤0.10 5.0-9.5 ≤1.0 13.0-17.0 ≥59.0 ≤10.0 1.0-2.5 ≤0.50 ≤1.0 ≤0.015 ≤0.030

IIPROPATHI ZOOMATSHINI EZIQHELEKILEYO ZONKE IZINSIMBI EZIWELDWELD

I-UTS YS Ukwandiswa Amandla empembelelo yeCVN (J) Ukwandiswa Kwamacala Amandla okuhambahamba kwi
(MPa) (MPa) (L= 5d)% kwiqondo lobushushu elingaphantsi kwe-196°C kwiqondo lobushushu elingaphantsi kwe-196°C (mm) 600°C kangangeeyure ezili-1000.
620 500 30 75 0.85 160 MPa

IDATHA EPHUMELELEYO NEYOKUPAKISHA: DC (+)

Ubungakanani (mm)

Ubude beDaya x

5×350

4×350

3.15×350

2.5×350

Uluhlu lwangoku (ii-Amps)

150-180

120-150

80-110

60-70

Ubunzima/Ibhokisi (iikhilogram)

2.5

2.5

2.5

2.5

Isilumkiso

1. Qinisekisa ukuba ii-electrode zomile. Zomise kwakhona ii-electrode kwi-300-325°C kangangeyure enye.

2. Gcina i-arc emfutshane, i-stringer bead kwaye unciphise ubushushu obungeniswayo.

3. Vumela i-weld iphole iye ngaphantsi kwama-50 C ngaphambi kokuba uyibeke, landela umaleko olandelayo.


  • Ngaphambili:
  • Okulandelayo: