I-AWS A5.18 ER70S-6 Ukuwelda kwentsimbi yekhabhoni Ukuzalisa iingcingo zesinyithi zokuwelda i-arc ekhuselweyo yigesi, iintambo eziqinileyo

Inkcazo emfutshane:

I-ER70S6 yintambo yokuwelda yentsimbi ethambileyo equlethe amanqanaba aphezulu e-manganese kunye ne-silicon kunezinye iintlobo eziqhelekileyo ze-MIG wire ukuya kwimveliso ye-welds esemgangathweni xa isetyenziswa kwintsimbi engcolileyo, enamafutha, okanye enomhlwa.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-ER70S6 yintambo yokuwelda yentsimbi ethambileyo equlethe amanqanaba aphezulu e-manganese kunye ne-silicon kunezinye iiklasi eziqhelekileyo ze-MIG wire ukuya kwimveliso ye-welds esemgangathweni xa isetyenziswa kwintsimbi engcolileyo, enamafutha, okanye enomhlwa. Umxholo ophezulu we-silicon unyusa ukunyibilika kwedama lokuwelda, ngaloo ndlela kudala ukubonakala okuthambileyo kweentsimbi kwaye kubangele ukugaywa okuncinci emva kokuwelda. Le ntambo yenzelwe ukubonelela nge-welds ezingena-porosity, ezikumgangatho we-x-ray ngamandla aphezulu okutsalwa (njengoko ziwelded) kuzo zonke iintambo zentsimbi yekhabhoni ezicacileyo.

Izicelo eziqhelekileyo: usetyenziso oluqhelekileyo lwevenkile olunezitya ezingasebenzi kakuhle okanye ezirhabaxa, iipleyiti ezinamafutha; ukwenziwa kwesinyithi okanye ukugcinwa kwezixhobo zokubumba; iiprojekthi zasekhaya; isinyithi; iitanki; umsebenzi wokwakha

Iklasi ye-AWS: ER70S6

Isiqinisekiso: AWS A5.18/A5.18M:2005

I-alloy: ER70S6

I-ASME SFA A5.18

Indawo yokuWelda: F, V, OH, H

Okwangoku: DCEP

Amandla okuThamba, kpsi:

70

Amandla okuvelisa, kpsi:

58

Ukwandiswa kwi-2”%:

22

I-Cystemi yeNtambo eqhelekileyo ngokwe-AWS A5.18 (amaxabiso alinganayo aphezulu)

C

Mn

Si

P

S

Ni

Cr

Mo

V

Cu

0.06-0.15

1.40-1.85

0.80-1.15

0.025

0.035

0.15

0.15

0.15

0.03

0.50

Iiparameters zeWelding eziqhelekileyo

Ububanzi

Inkqubo

I-Volt

Isantya Sokuhamba

Ii-Amps

Igesi yokukhusela

in

(mm)

(ipm)

.035

(0.9)

I-GMAW

23-26

11-22

160-300

Ukudluliselwa kweSpray 98% Argon+2% Oxygen

.045

(1.2)

I-GMAW

23-29

12-21

170-375

Ukudluliselwa kweSpray 98% Argon+2% Oxygen

1/16

(1.6)

I-GMAW

25-31

9-19

275-475

Ukudluliselwa kweSpray 98% Argon+2% Oxygen

.023

I-GMAW

14-19

10-15

30-85

Ukudluliselwa kweSekethe emfutshane 98% Argon+2% Oxygen

.030

(0.8)

I-GMAW

15-20

12-24

40-130

Ukudluliselwa kweSekethe emfutshane 98% Argon+2% Oxygen

.035

(0.9)

I-GMAW

16-25

11-40

60-235

Ukudluliselwa kweSekethe emfutshane 98% Argon+2% Oxygen

.045

(1.14)

I-GMAW

18-23

12-22

90-290

Ukudluliselwa kweSekethe emfutshane 98% Argon+2% Oxygen

.035

(0.9)

I-GTAW

12-15

N / A

60-100

I-Argon eyi-100%

.045

(1.14)

I-GTAW

13-16

N / A

70-120

I-Argon eyi-100%

1/16

(1.6)

I-GTAW

12

N / A

100-160

I-Argon eyi-100%

1/16- 3/32

(1.6)-(2.4)

I-GTAW

12

N / A

120-250

I-Argon eyi-100%

1/8

(3.2)

I-GTAW

12

N / A

150-300

I-Argon eyi-100%