Ni327-6 Nickel Alloy Welding Electrodes AWS A5.11 ENiCrMo-6 Welding Rods, Welding Structural Arc Welding Stick Electrodes

Inkcazelo emfutshane:

I-Ni327 -6 (AWS A5.11 ENiCrMo-6) i-electrode esekelwe kwi-nickel ene-low-hydrogen sodium coating.Sebenzisa i-DCEP (i-electrode yangoku echanekileyo).


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Nickel kunye ne-Nickel Alloy Welding Electrode

Ni327-6                                                     

GB/T ENi6620

I-AWS A5.11 ENiCrMo-6

Inkcazo: I-Ni327 -6 yi-electrode esekelwe kwi-nickel ene-low-hydrogen sodium coating.Sebenzisa i-DCEP (i-electrode yangoku ngqopositive).Intsimbi egciniweyo ineplastiki egqwesileyo, ukuqina kunye nokumelana nokuqhekeka.Isinyithi esibekiweyo sinomgca wokwandiswa kwe-coefficient efana naleyo yentsimbi, kwaye inamandla aphezulu kunye nokuxhathisa okuqinileyo kwi-corrosion kwiqondo lokushisa kunye nobushushu obuphezulu.

Isicelo: Isetyenziselwa ukuwelda kwentsimbi ye-Ni9%, kwaye ingasetyenziselwa ukuwelda kweentsimbi ezingafaniyo kunye ne-alloys enzima uku-weld.

 

Ukwakhiwa kweekhemikhali zentsimbi edibeneyo(%):

C

Mn

Si

Ni

Mo

Fe

Cu

≤0.10

2.0 ~ 4.0

≤1.0

≥55.0

5.0 ~ 9.0

≤10.0

≤0.5

Nb + Ta

W

Cr

S

P

Okunye

 

0.5 ~ 2.0

1.0 ~ 2.0

12.0 ~ 17.0

≤0.015

≤0.020

≤0.5

 

 

Iimpawu zobuchwephesha bentsimbi ye-weld:

Into yovavanyo

Tensile strength

Mpa

Unikeze Amandla

Mpa

Elongation

%

Iqinisekisiwe

≥620

≥350

≥32

 

yangoku eCetyisiweyo:

Intonga yobubanzi

(mm)

2.5

3.2

4.0

Welding okwangoku

(A)

50 ~ 70

80 ~ 100

110 ~ 150

 

Isaziso:

1. I-electrode kufuneka ibhakwe iyure enye malunga ne-300 ℃ phambi kokusebenza kwe-welding.Zama ukusebenzisa i-arc emfutshane ukuwelda;

2. Kubalulekile ukucoca umhlwa, i-oyile, amanzi, nokungcola kwiindawo zokuwelda phambi kokuba udiye.

3. Zama ukusebenzisa amandla omgca omncinci xa udibanisa, i-multi-layer kunye ne-multi-pass welding.

 

 


  • Ngaphambili:
  • Okulandelayo: