Ii-AWS A5.4 E308L-16 zokuWelda zentsimbi engagqwaliyo ii-electrode ze-arc zokuWelda ii-rod

Inkcazo emfutshane:

I-A002 (AWS E308L-16) yi-electrode yentsimbi engagqwali ye-Cr19Ni10 enekhabhoni ephantsi kakhulu ene-titanium-calcium coating.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Electrode yokuWelda yeNtsimbi engaGciniyo

A002                                                 

I-GB/T E308L-16

I-AWS E308L-16

Inkcazo: I-A002 yi-electrode yentsimbi engagqwali ye-Cr19Ni10 enekhabhoni ephantsi kakhulu ene-titanium-calcium coating. Ingasetyenziselwa zombini i-AC kunye ne-DC enentsebenzo entle yenkqubo. Umxholo wekhabhoni wesinyithi esigciniweyo yi-≤0.04% ebonelela ngentsebenzo entle yokulwa nokugqwala phakathi kwe-granular.

Ukusetyenziswa: Isetyenziselwa ukuwelda izakhiwo zentsimbi engagqwali ze-Cr19Ni10 ezinekhabhoni ephantsi kakhulu, kwaye ingasetyenziselwa izakhiwo zentsimbi engagqwali ze-06Cr18Ni1Ti ezimelana nokugqwala ezinobushushu obuphantsi kune-300°C; isetyenziselwa kakhulu ukwenza iifayibha zokwenziwa, izichumisi zeekhemikhali, ipetroliyam kunye nezinye izixhobo.

 

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

9.0 ~ 11.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Iimpawu zoomatshini zesinyithi esijijekileyo:

Into yovavanyo

Tensile strength

I-Mpa

Ukwandiswa

%

Iqinisekisiwe

≥520

≥35

 

I-current ecetyiswayo:

Ububanzi bentonga

(mm)

2.0

2.5

3.2

4.0

5.0

Ukuwelda kwangoku

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Isaziso:

1. I-electrode mayibhakwe iyure e-1 malunga ne-150℃ ngaphambi kokuba isebenze nge-welding;

2. Sebenzisa umbane we-DC kangangoko unako, kwaye umbane akufuneki ube mkhulu kakhulu ukuze kuthintelwe ukuba bomvu kwentonga yokuwelda;

3. Ukumelana nokugqwala kunye nomxholo we-ferrite wesinyithi esigciniweyo kumiselwa kukuvumelana kabini kokubonelela kunye nemfuno.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besisenza ushishino lokuvelisa ii-electrode zokuwelda, iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.


  • Ngaphambili:
  • Okulandelayo: