Ii-electrode zentsimbi engagqwaliyo ze-AWS E309MoL-16 ze-carbon ephantsi ze-Cr23Ni13Mo2 ze-Arc Welding, ii-Tyue Best Welding Rods

Inkcazo emfutshane:

I-A042(AWS E309MoL-16) yi-electrode yentsimbi engagqwaliyo ye-Cr23Ni13Mo2 enekhabhoni ephantsi kakhulu ene-titanium calcium coating.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Ukuwelda kweNsimbi EngagqwaliyoI-electrode

A042                                         

I-GB/T E309MoL-16

I-AWS E309MoL-16

Inkcazo: I-A042 yi-electrode yentsimbi engagqwali ye-Cr23Ni13Mo2 enekhabhoni ephantsi kakhulu ene-titanium calcium coating. Ingasetyenziselwa zombini i-AC kunye ne-DC. Ngenxa yokongezwa kwesixa esifanelekileyo se-molybdenum, ukumelana nokuqhekeka kunye nokumelana nokugqwala kwesinyithi esigciniweyo kuyaphucuka.

Isicelo: Kwizinto ezifanayo zentsimbi engenasici enekhabhoni esezantsi kakhulu (ezifana ne-urea synthesis tower lining) kunye ne-welding yentsimbi eyahlukileyo, njl.

 

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Iimpawu zoomatshini zesinyithi esijijekileyo:

Into yovavanyo

Tensile strength

I-Mpa

Ukwandiswa

%

Iqinisekisiwe

≥520

≥25

 

I-current ecetyiswayo:

Ububanzi bentonga

(mm)

2.5

3.2

4.0

5.0

Ukuwelda kwangoku

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Isaziso:

1. I-electrode mayibhakwe iyure e-1 malunga ne-150℃ ngaphambi kokuba isebenze nge-welding;

2. Ngenxa yokuba ubunzulu bokungena bungaphantsi kakhulu ngexesha lokuwelda nge-AC, umbane we-DC kufuneka usetyenziswe kangangoko ukuze ungene nzulu. kwaye umbane akufuneki ube mkhulu kakhulu ukuze kuthintelwe ukubomvu kwentonga yokuwelda;

3. Ukumelana nokugqwala kwesinyithi esigciniweyo kugqitywa kukuvumelana kabini kokubonelela kunye nemfuno.

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasungulwa ngo-2000. Besibandakanyeka kwimveliso yei-electrode yokuweldas, iintonga zokuweldakunyeizinto ezisetyenziswayo zokuweldakangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.