Ii-electrode ze-AWS E7014 ze-Carbon Steel Welding J501Fe ezithambileyo ze-Mild Steel Welding Rods

Inkcazo emfutshane:

I-J501Fe (AWS E7014) yi-iron powder kunye ne-titanium oxide electrode egqunywe yi-electrode.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Electrode yokuWelda yentsimbi yeCarbon

J501Fe

I-GB/T E5014

I-AWS A5.1 E7014

Inkcazo: I-J501Fe yi-electrode egqunywe yi-iron powder kunye ne-titanium oxide. Ingasetyenziselwa ukuwelda kwindawo yonke nge-AC kunye ne-DC, ukusebenza kakuhle kwe-deposition kumalunga ne-110%.

Isicelo: Kwizakhiwo zentsimbi yekhabhoni kunye nentsimbi ephantsi ye-alloy, ezifana ne-Q345 kunye nezinye iinqanawa, izithuthi kunye nezakhiwo zoomatshini zokuwelda.

Ukwakheka kweekhemikhali zesinyithi esijiyiweyo (%):

C

Mn

Si

S

P

≤0.12

≤1.25

≤0.60

≤0.035

≤0.035

 

Iimpawu zoomatshini zesinyithi esijijekileyo:

Into yovavanyo

Tensile strength

I-Mpa

Unikeze Amandla

I-Mpa

Ukwandiswa

%

Ixabiso lempembelelo (J)

0℃

Iqinisekisiwe

≥490

≥400

≥17

≥27

Ivavanyiwe

520 ~ 580

≥410

17 ~ 26

50 ~ 100

 

Ukuhlolwa kwe-X-ray: Ibanga lesi-II

I-current ecetyiswayo:

Ububanzi bentonga

(mm)

2.0

2.5

3.2

4.0

5.0

5.8

Ukuwelda komsinga

(A)

40 ~ 70

70 ~ 90

90 ~ 130

160 ~ 210

210 ~ 250

260 ~ 310

 

I-Wenzhou Tianyu Electronic Co., Ltd. yasekwa ngo-2000. Besisenza ushishino lokuvelisa ii-electrode zokuwelda, iintonga zokuwelda, kunye nezinto ezisetyenziswayo zokuwelda kangangeminyaka engaphezu kwama-20.

Iimveliso zethu eziphambili ziquka ii-electrode zokuwelda zentsimbi engagqwaliyo, ii-electrode zokuwelda zentsimbi yekhabhoni, ii-electrode zokuwelda ze-alloy ephantsi, ii-electrode zokuwelda eziphezu komhlaba, ii-electrode zokuwelda ze-nickel kunye ne-cobalt alloy, ii-wire welding zentsimbi emild kunye ne-low alloy, ii-wire welding zentsimbi engagqwaliyo, ii-wire ze-flux cored ezikhuselwe yigesi, ii-wire welding ze-aluminium, ii-inferiored arc welding. ii-wire, ii-wire welding ze-nickel kunye ne-cobalt alloy, ii-wire welding ze-brass welding, ii-wire welding ze-TIG kunye ne-MIG, ii-electrode ze-tungsten, ii-electrode ze-carbon gouging, kunye nezinye izixhobo zokuwelda kunye nezinto ezisetyenziswayo.

 

 


  • Ngaphambili:
  • Okulandelayo: