Inkcazo emfutshane:

I-AWS E6011i-electrode yokuweldaluhlobo lwe-cellulose potassium, esetyenziselwa ukuwelda okuthe tye. Zombini ukuwelda kwe-AC kunye ne-DC.


Iinkcukacha zeMveliso

Iithegi zeMveliso

Isicelo
Iintambo zokuwelda ze-AWS E6011 zifanelekile kwizakhiwo zeenqanawa zokuwelda ezifana nezakhiwo kunye neebhulorho, iitanki zokugcina izinto, iipayipi kunye nezixhobo zeenqanawa zoxinzelelo.

I-AWS E6011i-electrode yokuweldaluhlobo lwe-cellulose potassium, esetyenziselwa ukuwelda okuthe tye. Kokubini ukuwelda kwe-AC kunye ne-DC. Isebenzisa ubuchwepheshe obuphambili bangaphandle kwaye ineempawu zobugcisa zokuwelda ezibalaseleyo. Ubude be-ARC kufuneka bulawulwe kuluhlu olufanelekileyo. Ayisiyo i-multilayers welding kunye ne-cover welding efanelekileyo.

Ulwakhiwo lweeKhemikhali (%)
C Mn Si S P
≤0.2 0.3-0.6 ≤0.22 ≤0.03 ≤0.04
Iipropati zoomatshini zesinyithi esigciniweyo
Into yoVavanyo I-Rm (N/mm2) I-Rel (N/mm2) I-A (%) KV2(J) 0℃
Ixabiso leSiqinisekiso ≥420 ≥330 ≥22 ≥47
Isiphumo Jikelele 485 380 24 86
Isalathiso sangoku (DC)
Ububanzi φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
I-Amperage 40 ~ 70 50 ~ 90 90 ~ 130 130 ~ 210 170 ~ 230

UHLOBO LWE-CURRENT: I-Direct Current Electrode Positive (DCEP) okanye i-AC

IINDLELA ZOKWENDLELA EZICETYISWAYO ZOKUWELDA:

Ubude be-Arc – Ubude obuphakathi (1/8” ukuya kwi-1/4”)

Iflethi – Hlala phambi kwedama uze usebenzise intshukumo encinci yokutshaya

I-electrode ethe tye – I-engile ijonge kancinci phezulu kwipleyiti

Ukunyuka ngokuthe nkqo – Indlela yokutshaya okanye yokuluka kancinci

Phantsi ngokuthe nkqo – Sebenzisa i-amperage ephezulu kunye nokuhamba ngokukhawuleza, uhlale uphambi kwechibi

Ngaphezulu – Hlala phambi kwedama uze usebenzise intshukumo encinci yokutshaya

Ingqwalasela:
1. Kulula ukuyityhila kumswakama, nceda uyigcine kwindawo eyomileyo.
2. Ifuna ukufudunyezwa xa iphakheji iphukile okanye ifunxwe bumswakama, ubushushu bokufudumeza bufanele bube phakathi kwama-70C ukuya kuma-80C, ixesha lokufudumeza lifanele libe phakathi kwe-0.5 ukuya kwiyure e-1.
3. Xa usebenzisa ii-electrode zokuwelda ze-5.0mm, kungcono ukusebenzisa amandla aphezulu, aphantsi, ukuze kuphuculwe ukusebenza kokuwelda.