I-electrode yokuwelda yentsimbi yekhabhoni ye-E6010

Inkcazo emfutshane:

I-E6010 yi-electrode yohlobo lwe-rutile-cellulosic sodium.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-AWS E6010 I-Electrode Yokuwelda Yentsimbi Ethambileyo

ISICELO:

Ifanelekile ukuwelda isakhiwo sentsimbi esiphantsi kwekhabhoni njengemibhobho, ukwakhiwa kweenqanawa kunye nebhulorho njl.njl.

UHLELO:

I-AWS A5.1 / ASME SFA5.1 E6010

I-JIS Z3211 D4310

IIMPAWU:

I-E6010 yi-electrode yohlobo lwe-sodium ye-rutile-cellulosic. Ingadityaniswa kwindawo yonke (ingakumbi kwindawo ethe nkqo-phantsi) nge-DC+ kuphela. Isebenza kakuhle kakhulu njenge-arc ezinzileyo, ukuchitheka kancinci, ukususa i-slag ngokulula kunye nokukwazi ukubuyela kwakhona njl. Ulawulo olungcono lwedama elinyibilikisiweyo, amandla e-arc aqinileyo kunye nokungena okunzulu kwindawo ethe nkqo-phantsi.

UKWAKHIWA KWEEKHEMIKHALI ZONKE IINTSIMBI EZIWELDS: (Ubunzima %)

Izinto C Mn Si S P Ni Cr Mo V
Iimfuno ≤0.20 0.3-0.6 ≤0.30 ≤0.035 ≤0.040 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Iziphumo eziqhelekileyo 0.09 0.48 0.23 0.020 0.025 0.030 0.035 0.005 0.004

IIPROPATHI ZOMKHANIKI ZONKE IINTSIMBI EZIWELDWELD:

Izinto Rm/MPa I-Rel/Rp0.2 /MPa I-A/% I-KV2 (-30℃) /J
Iimfuno ≥430 ≥330 ≥20 ≥27
Iziphumo eziqhelekileyo 475 400 26 80

Ingqalelo:

1. Ngokubanzi, akufuneki uphinde uyomise i-electrode ngaphambi kokuba uyidibanise. Xa ichaphazeleka kukufuma, yiphinde uyomise kwi-70℃-90℃ kangangeyure e-1.

2. Umhlwa, ioyile, amanzi kunye nezinye izinto ezingcolileyo kwindawo yokuwelda kufuneka zisuswe ngaphambi kokuba ziwelding.

IINKQUBO ZOKUSEBENZA EZIQHELEKILEYO: (DC+)

Ububanzi (mm) 2.5 3.2 4.0 5.0
Ubude (mm) 300 350 400 400
I-current (A) 50-80 60-100 100-140 140-180

UKUPAKISHA:

5kg/ibhokisi, iibhokisi ezi-4/ibhokisi, 20kgs/ibhokisi, 50iibhokisi/ipalethi. 21MT -26MT nge-1X20″ FCL nganye.

 

I-OEM/ODM:

Sixhasa i-OEM/ODM kwaye singenza ukupakisha ngokwendlela oyila ngayo, nceda unxibelelane nathi ukuze sixoxe ngeenkcukacha.

 

Iimpawu zokusetyenziswa:

I-arc ezinzile kakhulu.

Ukususwa kakuhle kwe-slag.

Ukungena akunzulu kangako.

Ukumelana kakuhle nobushushu kunye nokugqwala.

Ukumelana kakuhle nokuqhekeka.